Nitrogen-Vacancy Centers in Fluorescent Nanodiamonds - Emerging Applications from Healthcare Diagnostics to Semiconductor Metrology
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Accounts of Chemical Research |
| Published | 2026-06-04 |
| Authors | Huan-Cheng Chang |
| DOI | 10.1021/acs.accounts.6c00047 |
A fluorescent nanodiamond thermography study cited in the Account localized an operating semiconductor hot spot with ±33 nm precision, compared with ±0.7 μm for lock-in infrared thermography. The Account links this result to three application classes: magnetically modulated immunoassays, extreme ultraviolet and soft X-ray scintillators, and wide-field device thermography with reported nanometer-scale spatial resolution and millisecond temporal resolution.
NV charge states and sensing signals
Section titled “NV charge states and sensing signals”Fluorescent nanodiamonds (FNDs) are monocrystalline diamond particles containing nitrogen-vacancy (NV) centers at concentrations of up to 10 ppm. Neutral NV⁰ and negatively charged NV⁻ are the most common states. Their zero-phonon lines occur at 2.156 eV and 575 nm for NV⁰ and 1.945 eV and 637 nm for NV⁻. The diamond band gap is 5.47 eV, and green excitation produces red fluorescence from both states.
The NV⁻ state can be optically polarized and coherently manipulated with microwave fields. Its triplet ground state has magnetic resonance transitions at 2.87 GHz. A 30 mT field can change bulk-diamond ensemble fluorescence by more than 10% when the field is neither aligned with nor perpendicular to the nitrogen-vacancy axis. Nanoscale NV⁻ centers retain this response, allowing lock-in detection to reject nonresonant background.
The charge-state distinction changes under high-energy excitation. Two-photon excitation at 344 nm produced fluorescence exclusively from NV⁰ in earlier work. Cathodoluminescence with 60 keV electrons produced similar NV⁰-selective behavior. This behavior supports using NV⁰ FNDs to convert EUV and soft X-ray radiation into visible light.
Spin-enhanced immunoassays
Section titled “Spin-enhanced immunoassays”Magnetic modulation made FND fluorescence detectable beneath the strong background of a nitrocellulose membrane. The immunoassay particles came from ion- or electron-bombarded monocrystalline high-pressure high-temperature diamond powders containing 100 to 200 ppm of neutral nitrogen impurities. At 532 nm excitation, their fluorescence intensity ratio was about 1:6 for NV⁰ and NV⁻. A 40 mT alternating field modulated FND fluorescence by more than 10%. Nitrocellulose modulation stayed below 0.005%, over 1000 times lower than the FND response. Magnetic modulation depth also exceeded the roughly 4% obtained with microwave modulation.
At 40 mT, a modulation frequency of 102.4 Hz, and a 30 s acquisition time, the detection limit for 100 nm FNDs was 0.04 ng/mm². This corresponded to 2 × 10⁴ particles/mm² for spherical particles. The sample could sit 5 mm from the electromagnet, and no photobleaching appeared during the measurement.
Before assay use, molten-salt treatment reduced particle size variation and surface roughness. The reported KNO3 treatment ran at 500 °C for 1 h. Dynamic light scattering gave a number-averaged hydrodynamic diameter of 93 nm and a polydispersity index of 0.093. Antibody or antigen conjugation and bovine serum albumin blocking increased the diameter by about 10 nm. The bioconjugates supported direct, competitive, and sandwich assay formats.
Sandwich spin-enhanced lateral flow immunoassays detected C-reactive protein, SARS-CoV-2 spike proteins, dengue virus nonstructural proteins, and markers for tuberculosis and Alzheimer’s disease. Typical antigen detection limits were 100 pg/mL when 100 μL of sample was applied. That matched the roughly 100 pg/mL limit specified for most commercial enzyme-linked immunosorbent assay kits. C-reactive protein below 1 μg/mL was detected with 3 μL of serum in a total assay time of 1 h.
EUV scintillators
Section titled “EUV scintillators”An electrosprayed FND film changed its fluorescence intensity by less than 2% after 1 h of continuous 60 nm EUV exposure at approximately 1 × 10¹¹ photons/s. Sodium salicylate decreased by more than 40% under the same conditions. The FND response was linear with beam flux, and temporal tests showed negligible afterglow.
At 13.5 nm, a CVD diamond containing 0.3 ppm of NV centers had a scintillation light yield of up to 7 photons/keV. Its fluorescence lifetime was less than 30 ns, compared with more than 100 ns for YAG:Ce. At that wavelength, penetration into diamond was only about 0.1 μm. These properties support fast, photostable conversion of EUV into visible fluorescence.
Bulk single-crystal plates were typically 3 × 3 mm² and 0.5 mm thick, which restricted beam-profile imaging. Electrospray deposition instead produced a uniform film about 1 μm thick over 10 × 10 mm² on indium tin oxide-coated glass. Film thickness varied by ±100 nm across the sample. Synchrotron tests covered 6.2 to 1200 eV, equivalent to 1 to 200 nm, and produced only NV⁰ fluorescence. The scintillator recorded gaseous O2 absorption spectra from 110 to 200 nm.
Fiber-coupled EUV imaging
Section titled “Fiber-coupled EUV imaging”Electrospray deposition applied FNDs to an indium tin oxide-coated fiber-optic plate for a compact imaging system. The plate measured 14 × 14 mm² and contained fused fibers with a 6 μm diameter. Its numerical aperture was 1, and its resolving power was 6 μm.
The fiber-coupled device achieved a noise-equivalent power density of 0.25 μW cm⁻² Hz⁻¹ᐟ², about 8 times lower than the lens-coupled system. It imaged synchrotron beam profiles from 300 to 1100 eV, producing images of 4.97 × 3.73 mm.
Operando semiconductor thermography
Section titled “Operando semiconductor thermography”Lock-in photoluminescence thermography achieved a calibrated photoluminescence response of −0.090%/K between 300 and 400 K. The test used a near-monolayer or approximately 100 nm FND film deposited by electrospray on a silicon wafer. Electrospray avoided uneven coverage caused by coffee-ring effects and particle aggregation during drop-cast solvent evaporation. Green excitation at 550 nm excited both NV⁰ and NV⁻ centers.
An inverted fluorescence microscope with autofocus correction maintained sample position during acquisition. Current pulses switched the device on and off. Fast Fourier transform analysis converted time-varying photoluminescence signals at each pixel into temperature-change images.
The proof-of-principle device was a P-channel vertical double-diffused field-effect transistor. A −60 V gate voltage was first applied to create defects, and the defective transistor then operated at a gate voltage of 20 V. Lock-in photoluminescence thermography detected the same hot spot as lock-in infrared thermography. The local temperature rise was about 10 times higher than in surrounding areas. The photoluminescence hot-spot profile had a full width at half-maximum of 30.3 ± 0.3 μm and peak localization precision of ±33 nm. The infrared profile measured 67 ± 2 μm and ±0.7 μm, respectively.
Continuous monitoring during transistor operation over 10 min gave an effective junction-to-ambient thermal resistance of 99 ± 1 °C/W. The Account treated this value as consistent with the manufacturer’s RθJA ≤ 292 °C/W specification and as evidence of measurement accuracy. The demonstrated camera system had a temporal resolution of 0.07 s, limited by its frame rate. The Account notes that lock-in cameras with response times as short as 20 μs could improve acquisition speed.
Engineering limits and material selection
Section titled “Engineering limits and material selection”Clinical use of the immunoassays still requires better surface attachment, less nonspecific binding, and improved reliability. The Account also calls for systematic evaluation of reproducibility, sensitivity, and specificity. Standardization and regulatory approval remain required before wider use in lateral-flow and microfiltration formats.
For EUV metrology, the sprayed films need better chemical stability and physical durability. The authors propose oxygen-plasma post-treatment to cross-link FND particles, remove organic contaminants, and regenerate clean surfaces. Quality-control and reproducibility tests are also needed.
For semiconductor thermography, spatial resolution is nearly 2 orders of magnitude better than infrared imaging, but temperature sensitivity is 10 times lower. The Account proposes higher frame rates for signal averaging. Material selection therefore follows the charge state and task. NV⁻ supports magnetic modulation and spin sensing, while NV⁰ provides the selective response used for EUV scintillation. Near-monolayer FND films support device thermography. The required material is NV-active FND rather than generic diamond.
Materials and support
Section titled “Materials and support”The Account’s EUV scintillator and semiconductor thermography use NV-active FND films on indium tin oxide-coated glass or a fiber-optic plate, including near-monolayer or approximately 100 nm coatings in the transistor test. 6CCVD’s diamond materials catalog lists MPCVD-grown single-crystal and polycrystalline diamond plates and wafers, with single-crystal thickness from 0.1 to 500 micrometers. Those plate formats meet the required thin-film scale, but an application-specific build still needs development of the electrosprayed particle coating, defect-generation route, and substrate integration through engineering support.
View Original Abstract
centers are quantum sensors capable of measuring temperature, magnetic, and electric fields at the nanoscale. These measurements are crucial for the design and evaluation of next-generation semiconductor devices. An innovative technique, termed FND-based lock-in photoluminescence thermography, has been developed to enable wide-field, real-time temperature mapping of actively operating devices such as bipolar junction transistors and field-effect transistors. The method achieves nanometer-scale spatial resolution and millisecond temporal resolution, yielding valuable insights into heat generation and dissipation processes in operando semiconductor devices.In summary, NV centers in FNDs constitute robust platforms for quantum sensing and metrology across a broad range of domains. From enhancing the sensitivity of immunodiagnostics to advancing EUV imaging and improving semiconductor thermal analysis, these quantum defects serve as transformative tools at the intersection of materials chemistry, biomedicine, and quantum technologies.
Single Crystal Cvd Diamond Plate
View Specs →
Electronic Grade Intrinsic Diamond Epitaxial Wafer H Terminated Superior 100 Mosfet Ready Substrate
View Specs →Cvd Diamond Coating On Silicon Wafer
View Specs →References we cover
Section titled “References we cover”Original source
Section titled “Original source”References
Section titled “References”- 2018 - Fluorescent Nanodiamonds [Crossref]