Transfer-printed yellow and red InGaN micro-LEDs on diamond for ultra-low-power high-speed optical interconnects
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Nature Communications |
| Published | 2026-06-17 |
| Authors | Runze Lin, Yu Zhang, Yucheng Yang, Shengyuan Dong, Handan Xu |
| DOI | 10.1038/s41467-026-74151-4 |
Transfer-printed 20 µm yellow InGaN micro-LEDs on passivated diamond reached an electrical-to-optical bandwidth of 2854.3 MHz at 25 A/cm². They retained 2850.4 MHz at 6.25 A/cm². The 20 µm red device reached 2617.7 MHz at 100 A/cm² and retained 2593.4 MHz at 50 A/cm². The 20 µm and 40 µm yellow devices also carried 1.5 Gbps over a 1 m fiber at 25 µA and 50 µA, with transmitter energy efficiencies of 0.056 pJ/bit and 0.110 pJ/bit.
Device design and low-current response
Section titled “Device design and low-current response”Superlattice strain management and a three-period quantum well design supported the low-current response. The authors grew the epitaxy by MOCVD on 4-inch Si (111) substrates. Ten pairs of low-indium InGaN/GaN superlattice strain release layers preloaded compressive strain in three high-indium InGaN/GaN quantum wells. The wells were 2.5 nm thick, and the barriers were 23.7 nm thick. The n-GaN electron transport layer was about 1.8 µm with Si doping above 1 × 10¹⁹ cm⁻³. The p-GaN hole injection layer had Mg doping above the same concentration.
The authors associated this structure with reduced quantum-confined Stark effect, blocked dislocation penetration, and faster carrier recombination within the active region. HAADF-STEM showed sharp, flat interfaces and no obvious dislocations in the red structure. EDS mapping showed relatively uniform indium across the quantum wells.
For bandwidth, the authors deliberately used defect-assisted nonradiative recombination in long-wavelength devices to deplete carriers faster at low injection. They treated this as an efficiency-for-bandwidth trade-off, while noting that the 20 µm yellow device kept a peak EQE of 2.50% at 1 A/cm².
Transfer printing and optical coupling
Section titled “Transfer printing and optical coupling”Fabrication used suspended mesas with one anchor and PDMS-stamp transfer printing. PDMS-A picked up the pixels, PDMS-B reversed their orientation, and PDMS-C deposited solder paste onto the target electrodes. Ti/Au electrodes were 30 nm/200 nm thick. The assembly was flip-chip bonded at 255 °C. Microscopy showed a flat, well-defined transfer onto diamond.
Two-photon lithography then formed the microlenses in place. The 20 µm emitter’s angular width at half peak intensity fell from 154.7° to 29.6°. The 40 µm device fell from 151.9° to 72°. The authors linked the stronger collimation of the smaller device to its lower emitter-area-to-lens-size ratio. Two-photon polymerization was chosen for proof-of-concept prototyping rather than array production.
Thermal role of diamond
Section titled “Thermal role of diamond”Diamond provided the heat-spreading path used to assess the emitters without early thermal limitation. Infrared camera measurements showed 20 µm yellow and red devices rising 6.6 °C and 6.7 °C on diamond at 6 mA. Their glass-substrate counterparts rose 84.1 °C and 90.0 °C at the same current. The measured values were surface hotspots, not junction temperatures.
The fitted temperature-rise coefficient of the 20 µm yellow device was 0.245 °C/mW on diamond and 3.057 °C/mW on glass. The diamond coefficient represented 8.01% of the glass value. The 40 µm yellow result was 0.064 °C/mW on diamond versus 3.289 °C/mW on glass. These data make bond-layer continuity and substrate heat spreading part of the high-speed device package.
Bandwidth across current density
Section titled “Bandwidth across current density”Bandwidth was measured with a 6 GHz vector network analyzer swept from 30 MHz to 3 GHz. The optical signal was detected with a 3 GHz photodetector before the S21 response was returned to the analyzer.
| Device | Current density | Electrical-to-electrical bandwidth (MHz) | Electrical-to-optical bandwidth (MHz) |
|---|---|---|---|
| 20 µm yellow | 25 A/cm² | 2383.3 | 2854.3 |
| 20 µm yellow | 6.25 A/cm² | 2135.8 | 2850.4 |
| 40 µm yellow | 15 A/cm² | 461.7 | 1148.3 |
| 20 µm red | 100 A/cm² | 1628.6 | 2617.7 |
| 20 µm red | 50 A/cm² | 1577.0 | 2593.4 |
| 40 µm red | 60 A/cm² | 277.8 | 1036.7 |
The cited prior maximum was 630 MHz for yellow micro-LEDs and 439.7 MHz for red micro-LEDs at 2 kA/cm². At 25 A/cm², the 20 µm blue, cyan, and green controls produced electrical-to-optical bandwidths of 107.6, 118.7, and 91.6 MHz. Their epitaxy used eight quantum wells, unlike the three-well yellow and red structures.
At 8 kA/cm², the 20 µm yellow and red devices reached electrical-to-optical bandwidths of 1659.7 and 2073.6 MHz. The blue, cyan, and green controls reached 677.8, 699.6, and 642.3 MHz at the same density. The authors attributed the low-current advantage to faster carrier depletion through nonradiative channels. At high injection, they associated the three-well design with higher carrier density and stronger radiative and Auger recombination terms.
Fiber link performance
Section titled “Fiber link performance”The OFDM link used a 1 m fiber and a 1600 MHz bandwidth. A 400 µm core silica multimode fiber had NA 0.22. A 1 GHz APD received the signal, and the data rate was selected against a 3.8 × 10⁻³ FEC threshold. At 32 mA for 20 µm devices and 80 mA for 40 µm devices, yellow rates were 4.74 and 6.35 Gbps. Red rates were 4.45 and 5.37 Gbps.
The low-power link used native OOK modulation without FFE or DFE. The rate was fixed at 1.5 Gbps because the 1 GHz detector limited higher rates. The 20 µm device used 25 µA at 6.25 A/cm² and 650 mV peak-to-peak drive. Its power was 84.0 µW at 3.360 V, giving 0.056 pJ/bit. The 40 µm device used 50 µA at 3.125 A/cm² and 650 mV peak-to-peak. Its power was 165.4 µW at 3.308 V, giving 0.110 pJ/bit.
A cited reference used a 470 nm blue device and reached 2.125 Gbps at 7.34 pJ/bit. The present yellow result had a lower rate but much lower transmitter energy per bit. Receiver power was excluded because the test used a commercial APD module and oscilloscope.
Limits for array integration
Section titled “Limits for array integration”Low-current operation exposed several unresolved issues. Near turn-on, the micro-LEDs showed nonlinear electrical-to-optical conversion, cutoff at lower current, and asymmetric eye diagrams. The red devices lacked the wideband SNR needed for microamp OOK capture on the oscilloscope. The reported energy figures cover only the transmitter.
At higher current, yellow emission shifted from 570.2 nm at 1 A/cm² to 487.9 nm at 8 kA/cm². Red shifted from 654.6 nm to 513.3 nm over the same current-density range. The authors judged these shifts acceptable for communication, but they would complicate fixed-spectrum or display use. Peak EQE remained low at 2.50% for yellow and 0.53% for red at 1 A/cm².
Array design still requires control of optical coupling, optical and electrical crosstalk, and matched detector arrays. The authors estimate 144 20 µm pixels could fit within 1 mm². Their projected aggregate rate is ~216 Gbps at 12.1 mW, but no such array was measured. They also identify sub-10 µm emitters as a route to looser fiber coupling and lower crosstalk. Two-photon lithography supports rapid prototyping, while nanoimprint lithography is proposed for larger arrays.
For diamond selection, the data support treating the substrate as an active heat-spreading element rather than passive support. Smaller mesas showed stronger self-heating at equal input power. Continuous heat flow through the bonding layer and into the diamond therefore matters for low-power and high-current operation.
Materials and support
Section titled “Materials and support”The study needs a passivated diamond plate for thermal management and flip-chip bonded yellow and red InGaN micro-LEDs, with patterned Ti/Au electrodes and solder bonding at 255 °C. 6CCVD’s diamond materials catalog lists MPCVD-grown single-crystal and polycrystalline diamond plates and wafers up to 125 mm. Because the paper leaves diamond type, thickness, size, surface finish, and bonding-layer specification open, engineering support should be used to match those requirements.
View Original Abstract
The rapid growth of computing demand requires high-speed transmission with low power consumption. Micro-light-emitting diodes (micro-LEDs), offering high modulation bandwidth, low-power operation, and array integration, are promising transmitters for next-generation interconnects. Here, we show yellow and red InGaN micro-LEDs, optimized through superlattice strain engineering and a three-period quantum well design, which were transfer-printed onto diamond, with microlenses fabricated by two-photon lithography for coupling optimization. The 20 µm yellow micro-LED achieved an electrical-to-optical bandwidth of 2850.4 MHz at 6.25 A/cm², while the 20 µm red device reached 2593.4 MHz at 50 A/cm². With on-off keying (OOK) modulation through a 1 m fiber link, 20 µm and 40 µm yellow devices achieved 1.5 Gbps at 25 µA (6.25 A/cm²) and 50 µA (3.125 A/cm²), with energy efficiencies of 0.056 pJ/bit and 0.110 pJ/bit, respectively. This study demonstrates the potential of InGaN yellow and red micro-LEDs for energy-efficient high-speed optical interconnects. The authors demonstrate transfer-printed yellow and red InGaN micro-LEDs on diamond substrates. These devices achieve a 1.5 Gbps data rate with an energy efficiency of 0.056 pJ/bit, enabling low-power, high-speed optical interconnects.
High Concentration Quantum Grade Single Crystal Diamond
View Specs →
Single Crystal Cvd Diamond Plate
View Specs →