High resolution microscopy and Raman Spectroscopic studies on the Freshest Mukundpura Meteorite, Rajasthan, India - Presence of nanodiamonds.
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Bulletin Of The Mineral Research and Exploration |
| Published | 2026-08-25 |
| Authors | D. Chandrasekharam, Govind Ummethala, Tripathi Rajendra Prasad, Amir Hossein Tavabi, Sairam K. Malladi |
| DOI | 10.19111/bulletinofmre.1795402 |
Raman spectroscopy supports the presence of nanocrystalline diamond with an average size of about 3 to 5 nm in the Mukundpura CM2 chondrite. The evidence includes a shifted diamond mode at 1320 cm^-1 and a weak feature near 1150 cm^-1. Broad carbon bands near 1360 and 1590 cm^-1 suggest disordered and graphitic carbon in the same matrix.
Nanodiamond occurrence in the CM2 matrix
Section titled “Nanodiamond occurrence in the CM2 matrix”The analyzed material is the CM2 carbonaceous chondrite that fell near Jaipur, Rajasthan, on 6 June 2017. The Geological Survey of India recovered about 2.2 kg of rock fragments. Its fall report described a pit 45 cm in diameter and 15 cm deep.
Previous thin section petrography assigned 15% to chondrules and 2% to opaque phases. Matrix formed the remainder, while sulfur-rich phases accounted for about 10% of the mesostasis. The current study selected a 1 cm chip from a granular area with an unusual concentration of crystalline carbon.
Sample preparation and measurement workflow
Section titled “Sample preparation and measurement workflow”Two separate chips were used because the SEM and TEM work took place in different laboratories. The authors doubly polished the SEM chip and gold coated it for analysis. A separate TEM chip was cut to about 5 mm, ground, polished, and gold coated.
| Method | Specimen condition | Main settings | Measurement |
|---|---|---|---|
| SEM-EDX | Doubly polished, gold-coated chip | JEOL JSM 7800 F; 20 kV; 0.17 nA; 10 mm working distance | Secondary electron imaging, EDS spectra, and elemental maps |
| Raman mapping | Carbon-rich area on the polished section | WITec alpha 300 R; 532.152 nm excitation; 50x/0.55 objective; about 5 μm laser spot | Two-dimensional intensity maps and carbon-phase Raman bands |
| TEM-EDX | Ground and polished chip about 5 mm, gold-coated | Titan G2 ChemiSTEM; 200 kV; HAADF imaging; 100 s per frame | Chondrule morphology, lattice imaging, and elemental mapping |
The methods list a Raman grid of 100 points per line and 100 lines per image. The mapped area was 50 μm by 50 μm, with 10 seconds per line and 0.1 seconds integration time. The results also describe a 140 μm by 80 μm scan that located a cluster of diamond particles.
Carbon-rich matrix and metal-rich phases
Section titled “Carbon-rich matrix and metal-rich phases”The SEM-EDX spectrum identified Fe-Mg-Ca silicates consistent with olivine and pyroxene. Carbon had the highest measured local fraction, at 58.9% atomic and 44.8 wt%. Sulfur measured 29.7% atomic and 30.1 wt%. Element maps showed carbon, oxygen, magnesium, silicon, sulfur, calcium, and iron distributed across the investigated region.
TEM-EDX identified nickel-rich chondrules and Fe-Ni-S pentlandite through the tested sample. Platinum lamellae cut across the matrix and Mg-Fe silicate chondrules. High-resolution TEM also showed large iridium grains. The authors discuss these grains in the context of impact-related iridium anomalies at stratigraphic boundaries.
These results provide a qualitative distribution of the matrix phases. The study reports no quantitative bulk concentration for iridium. The EDX percentages therefore describe the analyzed region rather than the composition of the full meteorite.
Raman assignment of 3 to 5 nm crystallites
Section titled “Raman assignment of 3 to 5 nm crystallites”| Raman feature | Position | Authors’ interpretation |
|---|---|---|
| Main diamond-related mode | 1320 cm^-1 | Shifted below the 1332 cm^-1 reference and asymmetric, consistent with nanocrystalline diamond |
| Broad lower band | About 1360 cm^-1 | Disordered carbon; deconvolution resolves 1320, 1360, and 1390 cm^-1 |
| Broad upper band | About 1590 cm^-1 | Graphitic carbon; deconvolution resolves 1562 and 1593 cm^-1 |
| Weak additional mode | About 1150 cm^-1 | Treated by the authors as evidence for nanocrystalline diamond |
The authors relate the shifted and asymmetric 1320 cm^-1 mode to reduced long-range order in nanometer crystallites. They state that symmetry breaking can shift and broaden the main 1332 cm^-1 mode. It can also create extra Raman features.
Their comparison with Raman data for 3 to 5 nm ultrananocrystalline diamond supports the size assignment. The Raman modes had low intensity. The authors attribute this to the small crystallite size and dilute concentration in the complex matrix. Raman mapping therefore provides the phase assignment, while electron microscopy establishes where the carbon-rich region occurs.
Comparison with reference spectra and prior meteorites
Section titled “Comparison with reference spectra and prior meteorites”The paper uses a 1332 cm^-1 peak with high intensity as the single-crystal diamond reference. The observed 1320 cm^-1 mode lies below that reference and is asymmetric. For graphitic carbon, the paper cites a 1575 cm^-1 G peak for single-crystal graphite and a 1355 cm^-1 D peak for disordered graphite. The observed broad regions near 1590 and 1360 cm^-1 support the presence of graphitic and disordered carbon alongside diamond.
Nanodiamonds had already been reported from stony and carbonaceous meteorites. The discussion compares Mukundpura with the Kapoeta meteorite and cites an approximate upper size of 400 μm. The paper does not reconcile that value with its 3 to 5 nm estimate for Mukundpura.
Formation interpretation and unresolved tests
Section titled “Formation interpretation and unresolved tests”The authors use the absence of a 1450 cm^-1 mode and the broadened, downshifted spectra to argue against shock-related diamond formation during or after the fall. They also cite no terrestrial weathering, no planar deformation features in olivine, and no major shock fabric. From these observations, they infer that the diamonds are inherent to the meteorite and formed in interstellar space. That origin is an interpretation because the present study reports no direct isotopic analysis of the diamonds.
Several measurement limits remain. The authors describe the elemental distribution as qualitative. The EDX percentages apply to the selected region, not the bulk sample. Quantitative elemental estimation remains in progress through atom-probe tomography.
The Raman size value is an average crystallite estimate. The study gives no particle size distribution. Selection of one 1 cm chip and a carbon-rich area does not establish the diamond abundance across the meteorite. The SEM and TEM datasets also refer to different chips.
The abstract reports the main vibrational mode at 1315 cm^-1, while the results and discussion place it at 1320 cm^-1. The paper does not explain this reporting difference.
Implications for diamond material selection
Section titled “Implications for diamond material selection”The study provides a reference for recognizing nanocrystalline diamond in a heterogeneous solid. The authors’ assignment relies on a shifted 1320 cm^-1 mode and a weak 1150 cm^-1 mode. The surrounding carbon still produces broad D and G regions, so the combined signature carries more information than one band alone.
The studied meteorite contains substantial non-diamond material. The mapped carbon occurs with sulfur, pentlandite, platinum, iridium, and silicate phases. The reported 3 to 5 nm value is an average Raman-based crystallite estimate. It is not a bulk purity value or a device specification.
The paper did not test engineered diamond or report optical, electrical, thermal, or mechanical performance. Device engineering would require separate measurements of phase purity, size distribution, and physical properties. Its contribution is a documented Raman signature for a natural CM2 matrix, not a manufacturing specification for engineered diamond.
View Original Abstract
Carbonaceous Chondrites have special significance in the stellar evolution and in particular in the evolution of life on earth. The carbonaceous meteorite that fell in Mukundpura village, Jaipur, Rajasthan on 6th June 2017 is one such rare CM2 carbonaceous meteorite. We carried out high resolution scanning and transmission electron microscopic studies on typical thin sections, showing abundant grains of iridium, pentlandite, and more interestingly crystalline carbon. These crystallite carbon grains resemble nanodiamond like signature in the freshest Mukundpura meteorite. The high-resolution Raman spectroscopic measurements are carried out on the crystalline carbon grains, showing well resolved three distinct peaks with a vibrational mode at 1315 cm-1, with the onset of a weak vibrational mode at 1150 cm-1, substantiating the observation of nanocrystalline diamond in Mukundpura meteorite. The broad peak centered at 1360 cm-1 and 1575 cm-1 (as an average), suggest the presence of graphitic carbon as well together with apparent presence of nanocrystalline diamond. The average size of nanocrystalline diamond is ~ 3-5 nm. High iridium content in this meteorite supports the meteoric impact related iridium anomaly in geological stratigraphic boundaries (e.g. Cretaceous-Tertiary boundary) that has caused mass extinction of flora and fauna.
High Concentration Quantum Grade Single Crystal Diamond
View Specs →
Single Crystal Cvd Diamond Plate
View Specs →