Skip to content

JUSTIFICATION OF DIAMOND DRILL BIT PARAMETERS FOR DRILLING MINERALIZED HARD ROCK

FieldValue
JournalNeft i gaz
Published2026-08-30
AuthorsBoranbay Ratov, Boris A. Fedorov, Aidar Kuttybayev, I.A. RUSLYAKOVA, Zamanbek Utepov
DOI10.37878/2708-0080/2026-4.04

The comparison calculation gives the proposed 95.6 mm diamond core bit 37.5% more footage per bit than a serial bit of the same type size, rising from 120 to 165 m. The same model raises mechanical drilling speed by 25%, from 1.0 to 1.25 m/h, and lowers specific breaking energy by 19.4%, from 18.0 to 14.5 kWh/m. These are calculated estimates for the developed design, not reported field-trial results.

The bit targets hard and especially hard rock containing dispersed or unevenly distributed useful minerals. Its outer diameter is 95.6 mm, and its recovered core diameter is 62 to 65 mm. The paper treats 62 to 63 mm as a satisfactory core diameter for unevenly mineralized ground and fixes the outer diameter at the standard 95.6 mm. Its comparative calculations use a core diameter of 63 to 64 mm.

Core size also depends on the final hole diameter, sampling reliability from recovered core, and the size of downhole instruments. The geological distribution of valuable material remains the main factor in choosing the core diameter. Uneven distribution is noted for rare metals, nonferrous and precious metals, mica, and asbestos.

The SU-95,6 bit has a threaded body for a core barrel or removable core catcher. Its working face combines PDC cutters with recessed, brazed cylindrical superhard elements placed close to them. PDC cutters use a hard-alloy body with a 0.5 to 0.6 mm polycrystalline diamond layer. The bit also includes flushing channels.

The cylindrical elements use a patented composite containing 22 to 25% diamond, 67 to 70% tungsten carbide, 4 to 4.5% cobalt, 1 to 2% chromium diboride, and 2 to 6% zirconium dioxide. The authors state that this composition and its manufacturing process produce a fine-grained structure with a strong matrix, high hardness, wear resistance, and cutting ability.

No hardness or wear values are reported for the composite. These material properties are therefore stated claims rather than independently tabulated test results.

The authors combine geological analysis, engineering analysis, theoretical modeling, and technical calculations. The rock-breaking calculation extends an earlier method for PDC drilling speed and for the chord length of a PDC segment contacting the rock. Its inputs include axial load, cutter count, rotational frequency, and rock mechanical properties. The model also defines cutter face angle, Schreiner rock hardness, and PDC chord length.

For gauge behavior, the authors derive equations from the helical motion of cylindrical gauge inserts during crown rotation and penetration. They relate insert diameter, inward projection, rotation time, and face advance to the rates at which the borehole wall and core are formed. All comparative calculations use the 95.6 mm outer diameter and the 63 to 64 mm core configuration.

The reported performance is a calculation and comparison exercise. The paper describes an experimental bit but does not report a field drilling campaign or laboratory measurement series for this design.

Each PDC cutter works beside a cylindrical composite element. Their end face and cutting edge lie in the same plane at the bottom of the hole. The calculation gives each member of a pair the same load P0, for a pair total of 2P0. The authors warn that axial load should be reduced at startup to prevent PDC breakage.

The cylindrical element acts first. Repeated contact with the face generates a crack zone under the PDC cutting edge. The weakened rock then separates more readily under the PDC cutter. This changes the sequence from cutting intact hard rock to pre-damaging and then cutting the same rock.

The authors attribute the speed and energy changes to this mechanism. They also attribute longer element life to load redistribution between PDC and cylindrical elements, which lowers stress concentration on individual PDC cutters. The fracture sequence and stress pattern were analyzed, not measured in the rock.

Radial cylindrical gauge inserts contact both the borehole wall and the core. As the crown rotates and advances, each insert follows a helical path. The derived relations connect insert diameter d, projection h, rotation period t, penetration rate, and gauge rate.

For inserts with equal diameter and equal inward projection, the model gives the same gauge rate for the borehole wall and core. The gauge rate must also exceed the rate at which the ring-shaped bottom advances. Under the adopted design, the calculated gauge rate exceeds bottom advance, which supports stable diameters during the run.

Poor matching can narrow the hole or enlarge the core. Either condition can trap the tool and end the drilling run. The model therefore links calibration to both diameter control and jam prevention.

Performance against the serial reference bit

Section titled “Performance against the serial reference bit”

The paper compares the developed bit with a serial diamond bit of the same type size.

Performance metricSerial bitDeveloped bitCalculated change
Mechanical drilling speed, m/h1.01.25+25%
Specific breaking energy, kWh/m18.014.5−19.4%
Footage per bit, m120165+37.5%
Wear intensity of cutting elements, mm/100 m1.61.1−31%

The comparison gives the developed bit 37.5% more footage per bit. Wear intensity falls by 31%, while mechanical speed rises by 25% and specific energy falls by 19.4%. The paper summarizes the footage result as an estimated 35 to 40% service-life gain. That gain is tied to reduced load concentration rather than an increase in the number of PDC cutters.

The comparison uses the same baseline for all four metrics. It does not provide a separate result for each rock class, so the values should not be treated as universal performance constants.

The main limitation is the evidence type. The paper provides analytical dependencies and calculated comparisons, but no test site, rock suite, hole depth, rotational speed, axial load, test duration, or uncertainty for the proposed bit. The serial reference is identified by type size only. Its geometry and operating record are not described in enough detail to reproduce the comparison.

The claims about core quality are also qualitative. The design aims to improve representativeness and conditions of core formation, but the paper reports no core-recovery percentage, contamination measurement, or sampling-bias metric. The same distinction applies to tool life. The 120 to 165 m comparison is a calculated estimate rather than observed run data.

For engineering use, the paper supports a 95.6 mm bit for recovering 62 to 65 mm core in hard mineralized rock. An operating procedure should lower axial load at startup and confirm that gauge formation can keep pace with penetration. Before assigning the modeled gains to a field campaign, operators should measure speed, energy, wear, and core recovery under representative geology.

The immediate conclusion is narrow: the paired diamond composite and PDC arrangement offers a calculable way to reduce breaking energy and distribute wear in a 95.6 mm mineral-exploration core bit.

View Original Abstract

The aim of this study is to provide a geological and technical justification for the parameters of a diamond core drill bit with an outer diameter of 95.6 mm and a core diameter of 62-65 mm, designed to improve the efficiency of core drilling in hard rock formations containing dispersed valuable minerals. The study included an analysis of the geological conditions governing the application of the drill bit, determination of the requirements for its design parameters, and investigation of the interaction between the rock-cutting elements and the rock mass. A technical justification was developed for the relative arrangement of a patented cylindrical diamond-containing element with high hardness and wear resistance and a polycrystalline diamond compact (PDC) cutter. The mechanism of rock fragmentation was investigated, whereby a highly fractured zone with reduced strength is first generated beneath the PDC cutter, after which the weakened rock is efficiently removed by the cutting elements of the drill bit. In addition, the process of gauge control of both the borehole wall and the recovered core was analyzed, taking into account the correspondence between their formation rate and the rate of rock destruction at the borehole bottom. The obtained results demonstrate that the proposed arrangement of the diamond-containing element and the PDC cutter intensifies the rock-breaking process by reducing the energy required for rock separation, improving the cutting efficiency of the drilling tool, and enhancing core formation conditions. The geological and technical justification of the proposed drill bit parameters supports its application in core drilling of hard rocks with dispersed mineralization, ensuring higher drilling productivity, increased tool service life, and improved quality of the recovered core. The proposed design is of both theoretical and practical significance for the development of high-performance drilling tools intended for geological exploration in hard rock formations.