Saturable absorption in NV-doped diamond studied by femtosecond Z-scan
Paper details
Section titled “Paper details”| Field | Value |
|---|---|
| Journal | Scientific Reports |
| Published | 2026-08-18 |
| Authors | Wojciech Talik, Mariusz Mrózek, Adam M. Wojciechowski, Krzysztof Dzierżęga |
| DOI | 10.1038/s41598-026-66816-3 |
| Citations | 1 |
NV-doped diamond displayed saturable absorption at 1032 nm, while a high-purity electronic-grade crystal displayed third-order nonlinear absorption. For the high-NV sample, weighted open-aperture Z-scan fits gave α₀ = 6.52 × 10⁻¹¹ cm⁻¹ and Iₛ = 40.0 GW/cm². The reconstruction supports H2 (NVN−) defects as the main source, although a weak NV contribution cannot be excluded. The H2 model yielded an effective dephasing time of 2.63 fs.
Samples and defect compositions
Section titled “Samples and defect compositions”Three commercial single-crystal diamonds separated lattice response from defect-driven response. The set included high-purity electronic-grade diamond, moderate-NV diamond, and high-NV diamond.
| Sample | N (ppm) | NV (ppm) | Size (mm³) | Face and edge orientation |
|---|---|---|---|---|
| EGSC | less than 0.005 | not listed | 2 × 2 × 0.5 | (001) and [110] |
| MCNV, DNVB1 | 0.8 | 0.3 | 3 × 3 × 0.5 | (001) and [100] |
| HCNV, DNVB14 | 13 | 4.5 | 3 × 3 × 0.5 | (001) and [100] |
MCNV and HCNV were made through nitrogen doping, electron irradiation, and annealing. NV centers therefore coexisted with substitutional nitrogen and aggregates including H2, H3, and N3V. Nitrogen concentrations were 0.8 and 13 ppm for MCNV and HCNV, respectively. Their NV concentrations were 0.3 and 4.5 ppm.
Linear spectra locate active transitions
Section titled “Linear spectra locate active transitions”Transmission was recorded from 200 to 1100 nm with 1.0 nm spectral bandwidth. Differential measurements placed HCNV in the signal arm and MCNV in the reference arm. This suppressed Fresnel reflections and geometric factors.
Second-derivative analysis then exposed weak and overlapping bands. The authors assigned three defects unambiguously from the spectra: H2 at 986 nm, NV− at 637 nm, and NV0 at 575 nm. A broad band near 550 nm was attributed to NV electronic and vibronic transitions. The 270 nm band was linked mainly to substitutional nitrogen. Features near 360, 419, and 520 nm were assigned to vacancy-related complexes, NVH defects, and N3 centers.
The EGSC spectrum remained featureless across the UV to NIR range, apart from the absorption edge below about 250 nm. Surface reflection losses dominated its transmission.
No feature appeared from 1042 to 1046 nm, suggesting a low metastable-state population. Features from 1020 to 1085 nm could not be assigned and may arise from irradiated defect structures. These findings placed 1032 nm inside a contested spectral region. The 1032 nm light therefore overlaps broad vibronic absorption bands rather than resonating with the principal zero-phonon lines.
Femtosecond open-aperture Z-scan
Section titled “Femtosecond open-aperture Z-scan”The laser supplied 230 fs pulses centered at 1032 nm, with photon energy 1.201 eV. The repetition rate was set to 1 kHz rather than the 10 MHz maximum. This reduced cumulative heating during repeated pulses.
A 10 cm focusing lens produced a 70 μm focal spot diameter and 7.3 mm Rayleigh range. The crystal moved along the beam axis through focus, changing the on-axis peak intensity. The open-aperture configuration measured intensity-dependent absorption without sensitivity to phase shift.
Identical large-area photodiodes recorded the transmitted and reference signals. Pulse energies came from integrating their temporal waveforms. Each measurement point was the mean of 500 shots and was normalized to the simultaneous reference detector.
Preliminary tests found no permanent optical or structural damage below 500 GW/cm². This threshold corresponded to pulse energies of about 2 μJ. All reported scans remained below that threshold, supporting an electronic origin for the measured response.
Undoped diamond shows nonlinear absorption
Section titled “Undoped diamond shows nonlinear absorption”The high-purity crystal showed nonlinear absorption instead of saturation. Its absorption coefficient followed α(I) = α₀ + βI. The fitted nonlinearity scaled linearly with peak intensity, identifying a third-order response.
The extracted coefficient was β = 4.9(3) × 10⁻¹⁵ m/W at 1032 nm. The authors considered direct two-photon absorption across the roughly 5.5 eV band gap unlikely. They attributed the response to deep impurity states or residual lattice defects at 1.201 eV photon energy.
NV-doped diamond shows saturable absorption
Section titled “NV-doped diamond shows saturable absorption”Both NV-doped crystals showed saturable absorption, and HCNV produced the stronger response. The fit used α(I) = α₀/(1 + I/Iₛ). For HCNV, weighted mean values from the fits gave α₀ = 6.52 × 10⁻¹¹ cm⁻¹ and Iₛ = 40.0 GW/cm².
Both parameters stayed largely independent of peak intensity within experimental uncertainty. Lower-intensity data deviated more from the fit. The authors linked those deviations to spatial heterogeneity and several coexisting defect types. The saturation model describes the overall trend rather than every measured point. Saturation strength increased with nitrogen and NV concentration.
H2 defects best explain the saturation
Section titled “H2 defects best explain the saturation”The effective two-level model treats each defect as ground and excited electronic states with phonon sidebands. The 1032 nm photon energy overlaps the broad H2 band despite detuning from its 986 nm zero-phonon line. That line corresponds to a resonance energy of 1.256 eV.
The analysis combined α₀, Iₛ, and a point-defect n₂ contribution from prior work, −0.758(56) × 10⁻²⁰ m²/W. Diamond’s refractive index at 1032 nm was 2.3904.
Assuming H2 dominated, the model gave an effective dephasing time T₂ = 2.63 fs. The reconstructed near-infrared spectrum had a similar shape to the measured absorbance. Its absolute amplitude was about twice the photometric value.
NV− and NV0 hypotheses required T₂ of about 0.15 to 0.2 fs. Their reconstructed spectral shapes did not match the measurement. The authors therefore identified H2 as the dominant source of saturation. A weak off-resonant NV contribution remained possible.
The 2.63 fs value is not a narrow-line coherence lifetime. It describes dephasing within a room-temperature vibronic band dominated by electron-phonon coupling. This corresponds to an effective linewidth of about 0.25 eV. Population relaxation contributes weakly to this effective dephasing under the model.
Limits and device implications
Section titled “Limits and device implications”Commercial NV crystals contain several defect species, so preparation alone cannot isolate H2. Low-intensity fit deviations show that one parameter set cannot describe every defect contribution. The reconstructed H2 absorbance exceeded the direct measurement by roughly a factor of two. These limits leave the exact NV contribution unresolved.
Direct defect-specific dephasing would require tunable Z-scan or wavelength-resolved pump-probe measurements. Neither was performed. The experiment also covered one excitation wavelength and pulse duration, so it does not map the saturation spectrum.
Earlier work on the same crystals used 230 fs pulses at 1032 nm and found positive n₂ with fourfold rotational anisotropy. NV-doped diamonds had lower n₂ than pure diamond in that Kerr study. Earlier Z-scan work at 800 nm examined near-surface NV effects on optical Kerr and two-photon absorption. Longer-wavelength work from 1200 to 1600 nm reported second-harmonic and cascaded third-harmonic generation.
The 1032 nm absorption result should not be generalized to every nonlinear observable in NV diamond. For high-power 1032 nm photonics, absorption saturation from the full defect population should be included in transmission models. An NV concentration label alone is insufficient. Linear spectra and the defect history should be considered.
Orientation remains relevant to Kerr engineering because the earlier response showed fourfold anisotropy. The present experiment does not establish orientation dependence for saturable absorption.
Materials and support
Section titled “Materials and support”The study needs NV-containing single-crystal diamond optical elements for femtosecond Z-scan transmission measurements. 6CCVD’s diamond materials catalog includes single-crystal diamond grown by MPCVD, supplied as plates and wafers, which matches the optical-element format. That entry does not specify NV concentration or the irradiation and annealing state that controls this response. Questions about defect composition and preparation requirements should go to engineering support.
View Original Abstract
Nonlinear optical absorption in commercially available diamond crystals containing nitrogen-vacancy (NV) centers is investigated using femtosecond open-aperture Z-scan measurements at a wavelength of 1032 nm. Experiments were performed on a high-purity electronic-grade diamond and on samples with moderate and high NV concentrations. While the undoped crystal exhibits third-order nonlinear absorption, the NV-doped samples show a pronounced saturable absorption response. To elucidate the microscopic origin of this effect, the Z-scan results are analysed in conjunction with linear transmission spectra, which reveal the presence of additional nitrogen-related defect complexes, including H2 ( (\hbox {NVN}^{-}) ) centers. Although the excitation wavelength is detuned from the principal zero-phonon lines of both NV and H2 defects, it overlaps with the broader near-infrared absorption band associated with vibronic transitions. A quantitative analysis based on an effective two-level model indicates that the observed saturable absorption is most consistently explained by a dominant contribution from H2 defects, while a weaker off-resonant contribution from NV centers cannot be excluded. The extracted parameters, including the linear absorption coefficient and saturation intensity, are supported by a reconstruction of the defect-related absorbance spectrum and by consistency with previously reported nonlinear refractive index data. These results highlight the importance of complex defect environments in determining the nonlinear optical response of NV-doped diamond and provide insight into defect-specific contributions relevant for diamond-based nonlinear and quantum photonic applications.
High Concentration Quantum Grade Single Crystal Diamond
View Specs →
Boron Doped Single Crystal Diamond Plate
View Specs →