DBR-free semiconductor disk lasers

MetadataDetails
Publication Date2015-01-01
AuthorsZhou Yang, Alexander R. Albrecht, Jeffrey G. Cederberg, Mansoor Sheik‐Bahae
InstitutionsUniversity of New Mexico, Sandia National Laboratories California

We demonstrate a novel DBR-free semiconductor disk laser, where multiple quantum well active region is fusion bonded directly onto a diamond heat spreader. CW output powers of 2.5 W have been demonstrated at 1150 nm.