Diamond-integrated optomechanical circuits
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-01-01 |
| Journal | Optical Fiber Communication Conference |
| Authors | Patrik Rath, S. Ummethala, Christoph E. Nebel, Wolfram H. P. Pernice |
| Institutions | Karlsruhe Institute of Technology |
Abstract
Section titled āAbstractāDiamond integrated photonic devices are promising candidates for applications in nanophotonics and optomechanics. Here I present active modulation of diamond-based devices by exploiting mechanical degrees of freedom in free-standing electro-optomechanical resonators.