Diamond Raman laser generating 25.5 fs pulses
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-01-01 |
| Journal | Advanced Solid-State Lasers |
| Authors | Jipeng Lin, David J. Spence |
| Institutions | Macquarie University |
Abstract
Section titled āAbstractāWe have demonstrated a 25.5 fs diamond Raman laser, which was synchronously-pumped by a 128 fs Ti:sapphire laser. The bandwidth of the Raman laser was significantly broadened by self-phase-modulation, with the effect maximized by compensating the intracavity dispersion using chirped mirrors.