Innovative hybrid heat sink materials with high thermal conductivities and tailored CTE
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-02-20 |
| Journal | Proceedings of SPIE, the International Society for Optical Engineering/Proceedings of SPIE |
| Authors | Michael Kitzmantel, Erich Neubauer |
| Institutions | University of Applied Sciences Technikum Wien, RHP Technology (Austria) |
| Citations | 7 |
Abstract
Section titled āAbstractāThis paper talks about high performance heat sinks and heat spreaders made by hybrid structures based on metaldiamond composites. Thermal conductivities can be tuned between 450 and 650 W/mK while maintaining customizable thermal expansion of 6-10 ppm/K (@30°C). Using different hybrid structures in combination with the metal-diamond core significant changes in thermal properties can be identified. Applications targeted are LED, disc laser and laser diode heatsinks with these high performance inserts without the need of CTE matched submounts.