The Dependence of the Thermophysical Properties of Filled Fluoroplastics on the Temperature and Concentration of Fillers
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2015-02-01 |
| Journal | International Polymer Science and Technology |
| Authors | Yu. P. Zarichnyak, V. A. Ivanov |
| Institutions | Russian Academy of Sciences |
| Citations | 2 |
Abstract
Section titled āAbstractāThe results of measuring the specific heat and thermal conductivity of composite materials based on a polytetrafluoroethylene matrix with different volume fractions of disperse fillers - powders of coke, molybdenum disulphide, and finely disperse diamonds - in the temperature range 200-550 K are presented.