Magnetic resonance tracking of fluorescent nanodiamond fabrication
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2015-03-25 |
| Journal | Journal of Physics D Applied Physics |
| Authors | Alexander I. Shames, V. Yu. Osipov, J.P. Boudou, A. M. Panich, H. J. von Bardeleben |
| Institutions | Centre National de la Recherche Scientifique, Physico-Technical Institute |
| Citations | 52 |
Abstract
Section titled âAbstractâMagnetic resonance techniques (electron paramagnetic resonance (EPR) and nuclear magnetic resonance (NMR)) are used for tracking the multi-stage process of the fabrication of fluorescent nanodiamonds (NDs) produced by high-energy electron irradiation, annealing, and subsequent nano-milling. Pristine commercial high pressure and high temperature microdiamonds (MDs) with mean size 150 Îźm contain ~5 Ă 1018 spins/g of singlet (S = 1/2) substitutional nitrogen defects P1, as well as sp3 C-C dangling bonds in the crystalline lattice. The half-field X-band EPR clearly shows (by the appearance of the intense âforbiddenâ g = 4.26 line) that high-energy electron irradiation and annealing of MDs induce a large amount (~5 Ă 1017 spins/g) of triplet (S = 1) magnetic centers, which are identified as negatively charged nitrogen vacancy defects (NVâ). This is supported by EPR observations of the âallowedâ transitions between Zeeman sublevels of the triplet state. After progressive milling of the fluorescent MDs down to an ultrasubmicron scale (â¤100 nm), the relative abundance of EPR active NVâ defects in the resulting fluorescent NDs (FND) substantially decreases and, vice versa, the content of C-inherited singlet defects correlatively increases. In the fraction of the finest FNDs (mean particle size <20 nm), which are contained in the dried supernatant of ultracentrifuged aqueous dispersion of FNDs, the NVâ content is found to be reduced by one order of magnitude whereas the singlet defects content increases up to ~2 Ă 1019 spins/g. In addition, another triplet-type defect, which is characterized by the g = 4.00 âforbiddenâ line, appears. On reduction of the particle size below the 20 nm limit, the âallowedâ EPR lines become practically unobservable, whereas the âforbiddenâ lines remain as a reliable fingerprint of the presence of NVâ centers in small ND systems. The same size reduction causes the disappearance of the characteristic hyperfine satellites in the spectra of the P1 centers. We discuss the mechanisms that cause both the strong reduction of the peak intensity of the âallowedâ lines in EPR spectra of triplet defects and the transformation of the P1 spectra.