Reducing GaN-on-diamond interfacial thermal resistance for high power transistor applications
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2015-03-16 |
| Journal | Applied Physics Letters |
| Authors | Huarui Sun, Roland B. Simon, James W. Pomeroy, Daniel Francis, Firooz Faili |
| Institutions | University of Bristol, Element Six (United States) |
| Citations | 207 |
| Analysis | Full AI Review Included |
Reducing GaN-on-Diamond Interfacial Thermal Resistance for High-Power Transistor Applications
Section titled “Reducing GaN-on-Diamond Interfacial Thermal Resistance for High-Power Transistor Applications”Executive Summary
Section titled “Executive Summary”- Core Achievement: Demonstrated a record-low effective thermal boundary resistance (TBReff) of 12 m2K/GW at the GaN-to-diamond interface, a critical bottleneck in high-power RF device thermal management.
- Primary Method: Utilized a contactless transient thermoreflectance technique coupled with finite element modeling and high-resolution TEM to isolate the specific contributions of the dielectric interlayer and the diamond nucleation zone.
- Key Finding: The TBReff is overwhelmingly dominated by the amorphous SiNx seeding layer and the defective diamond nucleation region. Minimizing these is the direct path to superior thermal performance.
- Actionable Result: By reducing the SiNx layer thickness from a standard ~100 nm down to the 28-34 nm range and optimizing the nucleation process, the team achieved a major reduction in overall transistor thermal resistance, outperforming standard GaN-on-SiC architectures.
- Material Validation: Confirmed that polycrystalline CVD diamond with a thermal conductivity reaching up to 2000 W/m·K is a viable, superior heat-spreading substrate for next-generation GaN HEMTs.
- Scalability: The study analyzed 17 distinct wafers produced via Hot Filament (HF) CVD and Microwave Plasma (MW) CVD methods, proving the robustness of the thermal optimization across different standard deposition techniques.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context & Application |
|---|---|---|---|
| Target Substrate | Polycrystalline CVD Diamond | — | Heat spreading layer for GaN HEMTs |
| Diamond Thermal Conductivity | Up to 2000 | W/m·K | Demonstrates the upper limit of the PCD heat spreader capability |
| Initial TBReff (Baseline) | 42 | m2K/GW | Measured on standard GaN-on-HF diamond with 100 nm SiNx layer |
| Optimized TBReff (Record) | 12 | m2K/GW | Achieved by minimizing SiNx thickness and nucleation defects |
| Minimum TBR Limit (Theoretical) | ~6 to 8 | m2K/GW | Approaching the Diffuse Mismatch Model (DMM) acoustic limit |
| GaN Layer Thickness | 0.7 - 1.0 | µm | Active device layer atop the diamond substrate |
| SiNx Interlayer Thickness | 28 - 100 | nm | Critical variable; thinner layers drastically reduce thermal resistance |
| Diamond Growth Thickness | 100 | µm | Bulk polycrystalline diamond layer |
| Measurement Technique | Transient Thermoreflectance | — | Contactless optical thermal probing |
| Heating Laser Specs | 355 nm, 10 ns pulse, 90 µm spot | nm / ns / µm | Nd:YAG frequency-tripled laser for thermal excitation |
| Probe Laser Specs | 532 nm CW, 2 µm spot | nm / µm | Nd:YAG frequency-doubled laser for reflectance monitoring |
| Acoustic Mismatch (Material Refractive Indices @ 532 nm) | nGaN ≈ 2.4, nSiNx ≈ 2.0, ndiamond ≈ 2.4 | — | Optical contrast utilized for interface measurement |
Key Methodologies
Section titled “Key Methodologies”The experiment followed a strict, multi-stage process to isolate and quantify the interfacial thermal resistance:
- Wafer Preparation (Template Fabrication):
- Started with an AlGaN/GaN heterostructure on a standard Si substrate (grown via MOCVD).
- Chemically/mechanically removed the Si substrate and intermediate nitride strain relief layers after mounting the active GaN onto a temporary handle wafer.
- Interlayer Deposition:
- Deposited an amorphous SiNx layer via low-pressure CVD (LPCVD) directly onto the exposed N-polar GaN surface.
- Varied the SiNx thickness precisely between 28 nm and 100 nm across the sample set to map thermal performance.
- Polycrystalline Diamond Growth:
- Utilized the SiNx layer as the seeding foundation for the CVD diamond.
- Employed two distinct reactor types for comparative analysis:
- Hot Filament (HF) CVD: Resulted in opaque wafers.
- Microwave Plasma (MW) CVD: Resulted in translucent wafers.
- Grew a thick diamond bulk layer (~100 µm).
- Thermal Characterization:
- Executed contactless transient thermoreflectance measurements using a 355 nm pulsed laser to induce rapid, localized heating.
- Monitored the subsequent surface cooling curve with a 532 nm CW probe laser.
- Microstructural Analysis & Modeling:
- Conducted Transmission Electron Microscopy (TEM) on the interfaces to physically correlate the nucleation defects with the measured thermal barriers.
- Applied finite element modeling to deconvolute the individual thermal resistance contributions (TBRSiNx vs. TBRnucleation).
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Connecting the findings of this research to the practical capabilities required to manufacture next-generation thermal management substrates:
-
Applicable Materials: To replicate or extend this research, clients require High Thermal Conductivity Polycrystalline Diamond (PCD). Specifically, our optical-grade and electronics-grade PCD wafers, featuring thermal conductivity ratings reaching 2000 W/m·K, are the ideal candidates to serve as the bulk heat-spreading layer described in this study. Given the study’s success with both HF and MW methods, our MPCVD-grown PCD is highly suitable for optimizing the nucleation density required to push TBReff toward the theoretical limit.
-
Customization Potential: The paper explicitly demonstrates that tuning the interfacial nucleation layer is key to performance. 6CCVD offers extensive custom fabrication services to meet these exact demands. We can provide custom metalization (including Ti, Pt, Au, and W stacks) to facilitate the hybrid integration of GaN epitaxial layers. Furthermore, 6CCVD provides custom dimensions up to 125mm for PCD plates, allowing for wafer-scale integration, along with precision laser cutting and polishing down to Ra < 5nm to ensure an optimal surface for the delicate seeding and CVD nucleation processes detailed in the paper.
-
Engineering Support: Achieving the record-low 12 m2K/GW thermal boundary resistance requires an exceptionally precise material specification. The 6CCVD in-house PhD engineering team is uniquely positioned to assist clients in selecting the exact PCD grade, thickness profile (we offer custom thicknesses from 0.1µm to 500µm), and nucleation surface morphology required for advanced GaN-on-Diamond RF amplifier and high-power transistor projects.
-
Call to Action: For custom specifications, advanced thermal interface material consultation, or to request a quote for your high-power electronics project, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Integration of chemical vapor deposited polycrystalline diamond offers promising thermal performance for GaN-based high power radio frequency amplifiers. One limiting factor is the thermal barrier at the GaN to diamond interface, often referred to as the effective thermal boundary resistance (TBReff). Using a combination of transient thermoreflectance measurement, finite element modeling and microstructural analysis, the TBReff of GaN-on-diamond wafers is shown to be dominated by the SiNx interlayer for diamond growth seeding, with additional impacts from the diamond nucleation surface. By decreasing the SiNx layer thickness and minimizing the diamond nucleation region, TBReff can be significantly reduced, and a TBReff as low as 12 m2K/GW is demonstrated. This enables a major improvement in GaN-on-diamond transistor thermal resistance with respect to GaN-on-SiC wafers. A further reduction in TBReff towards the diffuse mismatch limit is also predicted, demonstrating the full potential of using diamond as the heat spreading substrate.