The Effect of Surface Treatments on the Bond Strength Between CAD/CAM Blocks and Composite Resin
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2015-07-27 |
| Journal | Journal of Prosthodontics |
| Authors | Mustafa DĂŒzyol, Ămer SAÄSĂZ, Nurdan Polat SaÄsöz, NilgĂŒn AkgĂŒl, Mehmet Yıldız |
| Institutions | AtatĂŒrk University |
| Citations | 82 |
Abstract
Section titled âAbstractâAbstract Purpose The aim of this study was to evaluate the microtensile bond strength of three computerâaided design/computerâaided manufacturing (CAD/CAM) blocks repaired with composite resin using three surface treatment techniques. Methods and Materials Three different CAD/CAM blocks were used in this study: (1) Lithium disilicate, (2) feldspar ceramic, and (3) resin nano ceramic. All groups were further divided into four subgroups according to surface treatment: control, roughened with bur (B); roughened with bur and 5% Hydrofluoric acid (HF); roughened with bur and sandblasting (HF); and roughened with bur and CoJet (C). After surface treatments on each group, a silane and bonding agent were applied, and ceramics were repaired with a nanoâhybrid composite. Then, the repaired ceramics were cut with a lowâspeed diamond saw for microtensile bond testing. Microtensile bond tests for 40 specimens per subgroup were carried out with a universal testing machine. The data were analyzed with ANOVA, Tukeyâs, and LSD at the 95% significance level. Results Mean bond strengths (MPa) of subgroups B, HF, S, and C were: 0, 29.8, 0, 23.3 for lithium disilicate ceramic; 26.4, 22.3, 22.4, 22 for feldspar ceramic; 54.8, 25.3, 42.1, 25.7 for resin nano ceramic. For subgroups B and S of lithium disilicate ceramics, bonding failed during specimen preparation. No significant differences were observed among all CoJet groups. In subgroups B and S, resin nano ceramics showed the highest bond strength. In feldspar groups, subgroup B showed higher bond strength than the other subgroups. Conclusion This study demonstrates that lithium disilicate porcelain blocks required etching for repairing with composite material. Surface treatments did not increase the bond strength in feldspar ceramic groups and reduced the bond strength in resin nano ceramic groups.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2013 - Preliminary evaluation of clinical effect of computer aided design and computer aided manufacture zirconia crown
- 2004 - Repair or replacement of amalgam restorations: decisions at a USA and a UK dental school