Skip to content

Accuracy in the measurement of magnetic fields using nitrogen-vacancy centers in nanodiamonds

MetadataDetails
Publication Date2016-01-08
JournalJournal of the Optical Society of America B
AuthorsHaroon Aman, Taras Plakhotnik
InstitutionsThe University of Queensland
Citations13

We have measured 10 and 20 mT magnetic fields using NV centers in nanodiamonds and have demonstrated that the accuracy of these measurements is about 20 μT. This value is an order of magnitude larger than the precision defined by random fluctuations in the measurements. The presented analysis indicates that the 20 μT systematic errors at such fields are intrinsic to the nanodiamonds. The possible reason for this error is coupling of NV centers with paramagnetic entities in the nanodiamonds such as other NV centers, C13, and N14 nuclei.