Strong Resonant Coupling between a Surface Acoustic Wave and a Diamond Nitrogen Vacancy Center

MetadataDetails
Publication Date2016-01-01
JournalConference on Lasers and Electro-Optics
AuthorsAndrew Golter, Thein Oo, Hailin Wang
InstitutionsUniversity of Oregon

Autler-Townes splitting is observed when a surface acoustic wave (SAW) is coupled resonantly to two excited-states of a diamond nitrogen vacancy (NV) center, demonstrating strong coherent interactions between the SAW and the NV center.