Diamond machining of steel molds for optical components

MetadataDetails
Publication Date2016-06-23
JournalAdvanced Optical Technologies
AuthorsRoland Bohr

Abstract The requirement of ultra precision diamond machining of lens molds in steel is identified. A solution for this type of machining is presented and results of such a machining in steel compared to standard milling and polishing process are shown.