AuthorsA S C Nave, Benoît Baudrillart, S. Hamann, Fabien Bénédic, G. Lombardi
InstitutionsCentre National de la Recherche Scientifique, Sorbonne Paris Cité
Citations10

In a distributed antenna array (DAA) reactor, microwave H2 plasmas with admixtures of 2.5% CH4 and 1% CO2 used for the deposition of nanocrystalline diamond films have been studied by infrared laser absorption and optical emission spectroscopy (OES) techniques. The experiments were carried out in order to analyze the dependence of plasma chemical phenomena on power and pressure at relatively low pressures, up to 0.55 mbar, and power values, up to 3 kW. The evolution of the concentration of the methyl radical, CH3, of five stable molecules, CH4, CO2, CO, C2H2 and C2H6, and of vibrationally excited CO in the first and second hot band was monitored in the plasma processes by in situ infrared laser absorption spectroscopy using tunable lead salt diode lasers (TDL) and an external-cavity quantum cascade laser (EC-QCL) as radiation sources. OES was applied simultaneously to obtain complementary information about the degree of dissociation of the H2 precursor and of its gas temperature. The experimental results are presented in two separate parts. In Part I, the first paper in a two-part series, the measurement of the gas (Tgas), rotational (Trot) and vibrational (Tvib) temperatures of the various species in the complex plasma was the main focus of interest. Depending on the different plasma zones the gas temperature was found to range between about 360 and 1000 K inside the DAA reactor (Nave et al 2016 Plasma Sources Sci. Technol. 25 065002). In Part II, the present paper, taking into account the temperatures determined in the first paper, the concentrations of the various species, which were found to be in a range between 1011 and 1015 cm−3, are the focus of interest. The influence of the discharge parameters power and pressure on the molecular concentrations has been studied. To achieve further insight into general plasma chemical aspects the dissociation of the carbon precursor gases including their fragmentation and conversion to the reaction products has been analyzed in detail.