Diamond-Graphite Nanoplatelet Surfaces as Conductive Substrates for the Electrical Stimulation of Cell Functions
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2016-12-21 |
| Journal | ACS Applied Materials & Interfaces |
| Authors | Nuno F. Santos, Mónica CicuĆ©ndez, T. Holz, VirgĆlia S. Silva, A.J.S. Fernandes |
| Institutions | University of Aveiro |
| Citations | 22 |
Abstract
Section titled āAbstractāThe nanocarbon allotropes constitute valid alternatives when designing control and actuation devices for electrically assisted tissue regeneration purposes, gathering among them important characteristics such as chemical inertness, biocompatibility, extreme mechanical properties, and, importantly, low and tailorable electrical resistivity. In this work, coatings of thin (100 nm) vertically aligned nanoplatelets composed of diamond (5 nm) and graphite were produced via a microwave plasma chemical vapor deposition (MPCVD) technique and used as substrates for electrical stimulation of MC3T3-E1 preosteoblasts. Increasing the amount of N<sub>2</sub> up to 14.5 vol % during growth lowers the coatingsā electrical resistivity by over 1 order of magnitude, triggers the nanoplatelet vertical growth, and leads to the higher crystalline quality of the nanographite phase. When preosteoblasts were cultured on these substrates and subjected to two consecutive daily cycles of 3 μA direct current stimulation, enhanced cell proliferation and metabolism were observed accompanied by high cell viability. Furthermore, in the absence of DC stimulation, alkaline phosphatase (ALP) activity is increased significantly, denoting an up-regulating effect of preosteoblastic maturation intrinsically exerted by the nanoplatelet substrates.