Fabrication and high temperature electronic behaviors of n-WO3 nanorods/p-diamond heterojunction
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-01-30 |
| Journal | Applied Physics Letters |
| Authors | Liying Wang, Shaoheng Cheng, Chengze Wu, Kai Pei, Yanpeng Song |
| Institutions | Jilin University, State Key Laboratory of Superhard Materials |
| Citations | 38 |
Abstract
Section titled āAbstractāThis work explores the temperature-dependent characteristic and carrier transport behavior of a heterojunction of n-WO3 nanorods (NRs)/p-diamond. The n-type WO3 NRs grown by the hydrothermal method were deposited on a p-type boron-doped diamond film. The p-n heterojunction devices showed good thermal stability and have rectification characteristic from room temperature up to 290 °C. With increasing temperature, the turn-on voltages were decreased, and the rectification ratios were relatively high. The calculated ideality factor of the device decreased monotonously with increased temperature. The carrier transport mechanisms at different applied bias voltages following Ohmic laws, recombination-tunneling, and space-charge-limited current conduction of the heterojunction are discussed depending on temperature.