High-NA Aberration-Corrected Raman Analysis of Femtosecond Bessel Beam Modification in Diamond
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2017-01-01 |
| Authors | Brian K. Canfield, Lloyd M. Davis |
Abstract
Section titled âAbstractâWe report femtosecond Bessel beam laser processing of diamond with high-NA aberration-corrected Raman analysis in order to create improved arrays of micron diameter columnar graphitized electrodes for use in advanced high-energy particle detectors.