Imaging a Quantum Emitter with a High-Numerical-Aperture Diamond Metalens
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-01-01 |
| Authors | Richard R. Grote, TzuāYung Huang, Sander A. Mann, David A. Hopper, Annemarie L. Exarhos |
| Institutions | University of Pennsylvania, Institute for Atomic and Molecular Physics |
Abstract
Section titled āAbstractāWe demonstrate a high-transmission efficiency, high-numerical-aperture metalens etched into the surface of single-crystal diamond for coupling to quantum emitters. Metalens performance is matched to full-field simulations, and photoluminescence from a single nitrogen-vacancy center is imaged.