Recent advances in free-standing single crystalline wide band-gap semiconductors and their applications - GaN, SiC, ZnO, β-Ga2O3, and diamond

MetadataDetails
Publication Date2017-01-01
JournalJournal of Materials Chemistry C
AuthorsMunho Kim, Jung‐Hun Seo, Uttam Singisetti, Zhenqiang Ma
InstitutionsUniversity of Illinois Urbana-Champaign, University at Buffalo, State University of New York
Citations260

Free-standing single crystalline semiconductor membranes have gained intensive attention over the last few years due to their versatile usage in many applications.