Boron Doped Diamond Paste Electrodes for Microfluidic Paper-Based Analytical Devices

MetadataDetails
Publication Date2017-03-06
JournalAnalytical Chemistry
AuthorsSiriwan Nantaphol, Robert B. Channon, Takeshi Kondo, Weena Siangproh, Orawon Chailapakul
InstitutionsTokyo University of Science, Colorado State University
Citations101

Boron doped diamond (BDD) electrodes have exemplary electrochemical properties; however, widespread use of high-quality BDD has previously been limited by material cost and availability. In the present article, we report the use of a BDD paste electrode (BDDPE) coupled with microfluidic paper-based analytical devices (μPADs) to create a low-cost, high-performance electrochemical sensor. The BDDPEs are easy to prepare from a mixture of BDD powder and mineral oil and can be easily stencil-printed into a variety of electrode geometries. We demonstrate the utility and applicability of BDDPEs through measurements of biological species (norepinephrine and serotonin) and heavy metals (Pb and Cd) using μPADs. Compared to traditional carbon paste electrodes (CPE), BDDPEs exhibit a wider potential window, lower capacitive current, and are able to circumvent the fouling of serotonin. These results demonstrate the capability of BDDPEs as point-of-care sensors when coupled with μPADs.