Progress of Diamond-like Carbon Films
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-03-01 |
| Journal | DOAJ (DOAJ: Directory of Open Access Journals) |
| Authors | QingāYun Chen, Shi Kai-min, Minhua Su, Lyu Hui-yi, Luo Yu |
| Citations | 2 |
Abstract
Section titled āAbstractāDiamond-like carbon(DLC) films had many unique and outstanding properties such as high thermal conductivity, high hardness, excellent chemical inertness, low friction coefficients and wear coefficients. The properties and combinations were very promising for heat sink, micro-electromechanical devices, radiation hardening, biomedical devices, automotive industry and other technical applications, more research and a lot of attention were attracted in recent years. The research progress of diamond-like films and the nucleation mechanism of film were summarized, and application prospect of DLC films were demonstrated. The aim of this paper is to provide insights on the research trend of DLC films and the industry applications.