Hybrid integration of diamond membranes with GaN waveguides
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-06-18 |
| Journal | Strathprints: The University of Strathclyde institutional repository (University of Strathclyde) |
| Authors | P. Hill, H. Liu, Erdan Gu, Martin D. Dawson, Michael J. Strain |
| Institutions | Photonics (United States) |
Abstract
Section titled āAbstractāThe nitrogen vacancy (NV) is a photostable emitter in diamond which is optically accessible at room temperature and a potential candidate for quantum information processing as a spin register. The challenge facing research today is the efficient collection and manipulation of the NVās emissions, such as by enhancing the zero phonon line transitions for a coherent spin-photon interface.Integrating diamond with other photonic materials would allow for resonant coupling of the defect centre to optical devices on large area photonic integrated circuits (PICs). Emitted photons collected by bus waveguides could then be guided elsewhere on chip for entanglement or measurements.This work focuses on integrating ultra-thin diamond membranes with GaN waveguide and resonator devices. Mode simulations (see Fig. 1(a)) show that light can be coupled significantly into and out of the membranes by this method. Membranes of < 200 nm have been fabricated using Ar-Cl2 etch recipes that cumulatively smooth the diamond over time; an r.m.s roughness value of 0.19 nm has been achieved.1 The smooth surface and ultra-low thickness allow a good conformation and strong bonding of the membrane to other materials. This should allow for the integration of diamond membranes with photonic integrated circuits as shown schematically in Fig. (b).Free standing ultra-thin diamond membranes can also be used in tuneable open access cavities - where a low mode volume and high Q factor are desired; 2 or as templates for fabricating diamond optical devices on non-native substrates.3
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal Sourceā- DOI: None