FEM thermal and stress analysis of bonded GaN-on-diamond substrate
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2017-09-01 |
| Journal | AIP Advances |
| Authors | Wenbo Zhai, Jingwen Zhang, Xudong Chen, Renan Bu, Hongxing Wang |
| Institutions | Xiāan Jiaotong University |
| Citations | 10 |
Abstract
Section titled āAbstractāA three-dimensional thermal and stress analysis of bonded GaN on diamond substrate is investigated using finite element method. The transition layer thickness, thermal conductivity of transition layer, diamond substrate thickness and the area ratio of diamond and GaN are considered and treated appropriately in the numerical simulation. The maximum channel temperature of GaN is set as a constant value and its corresponding heat power densities under different conditions are calculated to evaluate the influences that the diamond substrate and transition layer have on GaN. The results indicate the existence of transition layer will result in a decrease in the heat power density and the thickness and area of diamond substrate have certain impact on the magnitude of channel temperature and stress distribution. Channel temperature reduces with increasing diamond thickness but with a decreasing trend. The stress is reduced by increasing diamond thickness and the area ratio of diamond and GaN. The study of mechanical and thermal properties of bonded GaN on diamond substrate is useful for optimal designs of efficient heat spreader for GaN HEMT.