Graphitization of a Polycrystalline Diamond under High-Fluence Irradiation with Noble Gas and Nitrogen Ions
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2017-11-01 |
| Journal | Journal of Surface Investigation X-ray Synchrotron and Neutron Techniques |
| Authors | Vasiliy Anikin, А. М. Борисов, В. А. Казаков, Е. С. Машкова, Andrey Morkovkin |
| Institutions | Moscow Aviation Institute, Lomonosov Moscow State University |
| Citations | 4 |
Abstract
Section titled “Abstract”To analyze the process of the ion-induced graphitization of a polycrystalline diamond, the surfacelayer conductivity and microstructure are studied experimentally after high-fluence irradiation with Ne+, Ar+, N+, and ions with energies of 20-30 keV at irradiation and heat-treatment temperatures ranging from 30 to 720°R in vacuum. After irradiation with argon ions at room temperature and subsequent heat treatment, the resistivity ϱ of a modified layer decreases exponentially with increasing treatment temperature T ht and reaches the graphite value ϱ at Tht = 700°R. Such a temperature T ht is insufficient for surface-layer graphitization by nitrogen ions. The increase in the diamond temperature under irradiation leads to a decrease in the ion-induced thermal graphitization temperature T g by several hundred degrees. It is found that the temperature T g is almost coincident with the corresponding temperature Ta of the dynamic annealing of radiation-induced damage in graphite. Analysis of the irradiated layer using Raman spectroscopy reveals the heterogeneous structure of the modified layer containing graphite and amorphous phases, the ratio between which correlates with the layer resistivity. Under argon-ion irradiation at diamond temperatures of 500°R or more, an increase in ϱ of the irradiated layer is observed, which is related to the formation of nanocrystalline graphite. This effect is not observed under nitrogen-ion irradiation.