Skip to content

Infrared and far-infrared magneto-spectroscopy of semiconductors in high magnetic fields in the megagauss range

MetadataDetails
Publication Date2017-12-07
AuthorsN. Miura
InstitutionsThe University of Tokyo

The recent progress of pulsed high magnetic field technology has made possible the IR and FIR spectroscopy under very high magnetic fields in the megagauss range (<100T), which opens up various new possibilities. In this paper, we present the latest results of the IR and FIR magneto- spectroscopy of semiconductors in the megagauss range, in particular, spectroscopy of novel interesting materials with low mobilities such as p-diamond, SiC, and AlAs, cyclotron resonance in a band with a camel’s back structure, and prominent polaron effects in II-VI compounds.