Intrinsically High Thermoelectric Performance in AgInSe2 n‐Type Diamond‐Like Compounds

MetadataDetails
Publication Date2017-12-18
JournalAdvanced Science
AuthorsPengfei Qiu, Yuting Qin, Qihao Zhang, Ruoxi Li, Jiong Yang
InstitutionsShanghai University, Shanghai Institute of Ceramics
Citations96

Abstract Diamond‐like compounds are a promising class of thermoelectric materials, very suitable for real applications. However, almost all high‐performance diamond‐like thermoelectric materials are p‐type semiconductors. The lack of high‐performance n‐type diamond‐like thermoelectric materials greatly restricts the fabrication of diamond‐like material‐based modules and their real applications. In this work, it is revealed that n‐type AgInSe 2 diamond‐like compound has intrinsically high thermoelectric performance with a figure of merit ( zT ) of 1.1 at 900 K, comparable to the best p‐type diamond‐like thermoelectric materials reported before. Such high zT is mainly due to the ultralow lattice thermal conductivity, which is fundamentally limited by the low‐frequency Ag‐Se “cluster vibrations,” as confirmed by ab initio lattice dynamic calculations. Doping Cd at Ag sites significantly improves the thermoelectric performance in the low and medium temperature ranges. By using such high‐performance n‐type AgInSe 2 ‐based compounds, the diamond‐like thermoelectric module has been fabricated for the first time. An output power of 0.06 W under a temperature difference of 520 K between the two ends of the module is obtained. This work opens a new window for the applications using the diamond‐like thermoelectric materials.