A 900-Watt quasi-CW diamond Raman laser

MetadataDetails
Publication Date2018-01-01
AuthorsSergei Antipov, Alexander Sabella, Soumya Sarang, Robert J. Williams, David J. Spence
InstitutionsMacquarie University, Defence Science and Technology Group
Citations1

A high beam quality diamond Raman laser operating in the quasi-CW regime with 900 W output power in 100 µs pulses was demonstrated above the modelled cavity stability limit. A 40Ɨ brightness enhancement was measured.