  • Material Innovation: First-principles exploration of the Si24 allotrope reveals an order-of-magnitude enhancement in thermoelectric figure of merit (ZT) over cubic diamond silicon (dSi) at room temperature.
  • Intrinsic Nanostructuring: Si24 contains an intrinsic array of nanosized pores, effectively scattering phonons (heat) while preserving electronic conduction—eliminating the need for extrinsic nanostructuring.
  • Doping Strategy: Light n-type doping (approximately 0.21 × 1020 cm-3) maximizes ZT via multiple valley degeneracy and an enhanced power factor.
  • Anisotropic Transport: Electrical and thermal conductivities display strong anisotropy (κl along z-axis is roughly 13× lower than dSi); engineering along specific crystallographic axes is critical.
  • Rattler Enhancement: Residual Na guest atoms within pores donate electrons and suppress phonon transport simultaneously, mimicking high-performance clathrate systems.
  • Computational Rigor: Calculations explicitly enumerate electron-phonon scattering and three-phonon anharmonicity without empirical relaxation times, ensuring predictive reliability.
  • Application Outlook: Si24 presents a thermally stable, non-toxic, Earth-abundant pathway to high-performance thermoelectric modules for waste-heat recovery.
ParameterValueUnitContext
ZT Enhancement (peak)Order-of-magnitude increase over dSi—At 300 K with light n-type doping
Optimal Doping~0.21 × 1020cm-3At 300 K, intrinsic + spontaneous Na doping
Lattice Thermal Conductivity (κl, x-axis)~4× lower than dSi—Across 300-800 K range
Lattice Thermal Conductivity (κl, z-axis)~13× lower than dSi—Across 300-800 K range
Power Factor (σS2)Maximized at light electron doping—Strong anisotropy; suppressed under hole doping
Electron-Phonon Relaxation (τn,ke-ph)Significantly longer than dSifsEspecially at low carrier energies
Predicted Doping Concentration (2 Na ions / 288 Si)~0.7at.%Threshold for donor level emergence
Single Na Doping Concentration (1 Na / 288 Si)~1.58 × 1020cm-3Spontaneous electron doping without band distortion
Electronic Plane Wave Cutoff60 Ry (816.34)Ry (eV)Used for electron-phonon matrix elements
k/q Grid (Coarse)10 × 10 × 6—Γ-centered Brillouin zone mesh
k/q Grid (Dense Interpolation)40 × 40 × 9—Used for transport coefficients; <5% error vs 50 × 50 × 9
Supercell for Anharmonic Phonons3 × 3 × 2 (216 Si atoms)—Finite displacement: 0.03 Å cutoff / 15 Å cutoff
VASP Kinetic Cutoff400eVHellmann-Feynman force evaluation
Vacancy / Interstitial Formation Energy2.3-3.7eVHigher than substitutional dopants
Substitutional Dopant Formation Energy<0.7eVIndicates easier incorporation
Guest Na Migration Barrier~1eVNudged elastic band (NEB) calculation
Si24 Thermal Stabilityup to ~750KConfirmed by Raman agreement
Si24 Pressure Stabilityup to ~8GPaConfirmed by experimental Raman
  • First-Principles Platform: DFT using Quantum Espresso (norm-conserving pseudopotentials, PBE-GGA exchange-correlation).
  • Electronic Transport: Boltzmann transport via Bolztrap with semi-classical formulation.
  • Electron-Phonon Coupling (Wannier Interpolation):
    • Compute gm,nk,λ matrix elements on a coarse 10 × 10 × 6 mesh.
    • Interpolate to dense 40 × 40 × 9 mesh via maximally localized Wannier functions (MLWFs).
  • Phonon Transport (Three-Phonon Scattering):
    • 3 × 3 × 2 supercell (216 Si atoms) with VASP (PAW, 400 eV cutoff).
    • 12,108 displaced configurations, 0.03 Å displacement cutoff, 15 Å interaction cutoff.
    • Solve Boltzmann transport equation using phono3py.
  • Defect/Dopant Evaluation: Formation energy calculations comparing substitutional vs. intrinsic point defects.
  • Guest Atom Migration: Nudged elastic band (NEB) for Na diffusion barrier determination.
  • Electronic Contribution to κ: Wiedemann-Franz law with L0 = 2.44 × 10-8 W·Ω/K2.

The pursuit of high-ZT thermoelectric materials—where high electrical conductivity must coexist with suppressed phonon transport—directly maps to a need for precisely engineered wafer surfaces and metallization architectures. The following outlines how 6CCVD’s diamond manufacturing capabilities support next-generation device prototyping in this field.

Research Requirement6CCVD Material
Non-toxic, thermally stable host matrix for high-temperature operation (~750 K)Optical Grade Single Crystal Diamond (SCD)
Anisotropic thermal/electrical conduction control via surface orientationSingle Crystal Diamond (SCD) with controlled crystallographic orientation (100 / 110 / 111)
Substrates for thin-film thermoelectric module integrationPolycrystalline Diamond (PCD) Plates (up to 125mm)
Heavily doped contact layers or sensing elementsHeavy Boron Doped Diamond (BDD) for conductive interfaces
Boron-doped carrier concentration control for optimal thermoelectric responseCustom Resistivity BDD (10-2 to 104 Ω·cm)
  • Surface Engineering: Si24 anisotropic κl differences (4× to 13× depending on the x/z axis) demand atomically smooth interfaces. 6CCVD delivers SCD polished to Ra &lt; 1 nm and inch-size PCD polished to Ra &lt; 5 nm, ensuring uniform thermal contact at boundary layers.
  • Thickness Control: The Si24 study emphasizes thin-film integration for electron and phonon transport validation. Our SCD and PCD thin-film capabilities span 0.1 µm to 500 µm, enabling freestanding or substrate-supported architectures.
  • Metallization: Thermoelectric device fabrication typically requires ohmic contacts (Ti/Pt/Au) and high-temperature electrodes. 6CCVD provides in-house metallization with Au, Pt, Pd, Ti, W, and Cu, optimized for adhesion on diamond surfaces.
  • Laser Cutting: Custom die geometries and micron-scale contact pads can be produced via laser micro-machining, matching the Si24 nanoporous architecture at the device level.

6CCVD’s in-house PhD team can assist with material selection for:

  • Thermoelectric module substrate engineering
  • High-temperature thermal management for Si24 layer integration (up to 750 K)
  • Boron-doped diamond as carrier-selective transport layers
  • Diamond metallization stack design for thermal/electrical interface engineering
  • Wafer-scale prototype fabrication for waste-heat recovery systems
ServiceSpecification
Wafer DimensionsUp to 125 mm diameter (PCD)
Thickness Range0.1 µm - 500 µm (SCD/PCD); up to 10 mm substrates
Surface RoughnessRa &lt; 1 nm (SCD), Ra &lt; 5 nm (PCD)
MetallizationAu, Pt, Pd, Ti, W, Cu (in-house)
MaterialsSCD, PCD, BDD (light to heavy doping)
ShippingGlobal DDU (DDP available)

Call to Action: For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

Thermoelectric device is a promising next-generation energy solution owing to its capability to transform waste heat into useful electric energy, which can be realized in materials with high electric conductivities and low thermal conductivities. A recently synthesized silicon allotrope of Si${24}$ features highly anisotropic crystal structure with nanometre-sized regular pores. Here, based on first-principles study without any empirical parameter, we show that the slightly doped Si${24}$ can provide an order-of-magnitude enhanced thermoelectric figure of merit at room temperature, compared with the cubic diamond phase of silicon. We ascribe the enhancement to the intrinsic nanostructure formed by the nanopore array, which effectively hinders heat conduction while electric conductivity is maintained. This can be a viable option to enhance the thermoelectric figure of merit without further forming an extrinsic nanostructure. In addition, we propose a practical strategy to further diminish the thermal conductivity without affecting electric conductivity by confining rattling guest atoms in the pores.