Skip to content

Enrichment of ODMR-active nitrogen-vacancy centres in five-nanometre-sized detonation-synthesized nanodiamonds - Nanoprobes for temperature, angle and position

MetadataDetails
Publication Date2018-03-26
JournalScientific Reports
AuthorsShingo Sotoma, Daiki Terada, Takuya F. Segawa, Ryuji Igarashi, Yoshie Harada
InstitutionsJapan Science and Technology Agency, The University of Osaka
Citations51
AnalysisFull AI Review Included
  • Breakthrough in Nanoscale Sensing: Demonstrates that 5 nm-sized detonation-synthesized nanodiamonds (DND-OH) retain nitrogen-vacancy center (NVC) functionality comparable to bulk diamond, enabling single-molecule-resolution biosensing.
  • Stable Negative Charge (NV-): Krüger’s surface reduction (hydroxyl termination) locks NVCs into a stable negatively charged state, a prerequisite for ODMR-based quantum measurements.
  • Record Coherence Time: Achieves T2 spin relaxation times of 1-4 µs (Hahn echo) at the 5 nm scale — the longest reported for sub-10 nm diamond particles.
  • Multimodal Sensing Capability: Validates three distinct applications — thermosensing (ΔD = −76 ± 13 kHz/K), one-degree orientation determination, and super-resolution imaging (33 nm separation between NVCs resolved).
  • Biocompatibility Validation: Proves suitability for intracellular measurements with particle dimensions comparable to green fluorescent protein (GFP).
  • FRET Compatibility: H3 (N-V-N) emission overlaps with NVC excitation, opening photostable Förster resonance energy transfer pathways for biomolecular proximity mapping.
  • Method: Thermal annealing at 800°C (vacuum, 2 h) followed by 425°C oxidation (5 h) and Krüger’s hydroxylation protocol.
ParameterValueUnitContext
DND Particle Size5.3 ± 1.0nmMean diameter (NanoAmando® precursor)
NVC Charge StateNV-—Stabilized negative charge
T2 Relaxation Time1-4µsHahn echo measurement at 5 nm scale
Rabi Oscillation Period~68nsReported resonance pulse width
ODMR Zero-Field Splitting (25°C)2868.65MHzResonance frequency
ODMR Zero-Field Splitting (45°C)2870.17MHzTemperature-shifted resonance
Temperature Sensitivity (ΔD)−76 ± 13kHz/KLinear thermosensing coefficient
Excitation Wavelength532nmNd:YAG laser
Laser Power100mWContinuous-wave illumination
Emission Filter Range590-845nmLong-pass detection window
Objective Magnification60× / 100×—1.49 NA oil-immersion
Microwave Sweep Range2670-3070MHzFrequency-sweep ODMR
Microwave Frequencies (Selective Imaging)2821 / 2857MHzTwo NVC discrimination
Super-Resolution Distance33nmTwo-NVC separation measured
Position Error (NVC 1 / NVC 2)11 / 7nmShot noise + instrument instability
Orientation Angles50° / 72°degreeNVC-to-field angles
Annealing Temperature800°CVacuum, 2 h (NVC creation)
Oxidation Temperature425°C5 h (graphite removal)
XRD Wavelength (Cu Kα)0.15405nm—
XRD Tube Voltage / Current30 kV / 30 mA——
FTIR Resolution2cm−1KBr pellet method
  • Step 1 — DND Colloid Preparation: Freeze-dry colloidal NanoAmando® solution (5.3 ± 1.0 nm); thermally anneal at 800°C for 2 h under vacuum to generate NVCs.
  • Step 2 — Graphite Removal: Oxidize at 425°C for 5 h to eliminate surface graphitic carbon (yielding DND-bare).
  • Step 3 — Surface Functionalization: Apply Krüger’s protocol for hydroxyl termination → DND-OH, stabilizing the NV- charge state.
  • Step 4 — Structural Verification:
    • TEM imaging (JEOL JEM-1011).
    • XRD with Cu Kα (0.15405 nm); acceleration 30 kV, current 30 mA.
    • FTIR (JASCO FT/IR 4200, 2 cm−1 resolution, KBr pellets).
    • Zeta-potential analysis (Malvern Zeta sizer Nano).
  • Step 5 — Confocal ODMR Setup:
    • 532 nm Nd:YAG excitation (100 mW).
    • EMCCD detection (Andor iXon DU897).
    • Oil-immersion objectives (60× / 100×, NA 1.49).
    • Dichroic mirror centered at 575 nm; band-pass 590-845 nm.
  • Step 6 — Pulse Measurements (Rabi & Hahn Echo): Rabi oscillation ~68 ns pulse; Hahn echo sequence confirms T2 = 1-4 µs.
  • Step 7 — Selective Super-Resolution Imaging: Microwave sweep 2670-3070 MHz; selective excitation at 2821 / 2857 MHz to resolve two NVCs separated by 33 nm.
  • Step 8 — Orientation & Temperature Calibration: External neodymium magnet enables orientation mapping (50° / 72°); temperature sweep confirms linear ΔD = −76 ± 13 kHz/K.

Applicable Materials

6CCVD Material GradeRelevance to This Research
Single Crystal Diamond (SCD)Reference bulk material for NVC baseline behavior and characterization.
Polycrystalline Diamond (PCD)Scalable alternative for ensemble NV sensing where large areas are needed.
Boron-Doped Diamond (BDD)Applicable where conductive substrates are required for spin-state electrical manipulation or MEMS-integrated ODMR.

For direct replication of this detonation-nanodiamond work, single-digit nanodiamond powders (5-10 nm) with controlled nitrogen vacancy density are required; for bulk thin-film or wafer-based extensions of NV magnetometry/thermometry, SCD and PCD wafers from 6CCVD provide the requisite lattice quality and dimensional control. Custom thickness down to 0.1 µm enables ultra-thin sensing membranes suitable for lab-on-chip integration.

Customization Potential

Parameter6CCVD Capability
Wafer DimensionsUp to 125 mm (PCD); custom geometries via laser cutting.
Thickness RangeSCD: 0.1-500 µm; PCD: 0.1-500 µm; Substrates up to 10 mm.
Surface FinishRa < 1 nm (SCD); Ra < 5 nm (inch-size PCD) — optical-grade flatness for evanescent-coupling ODMR geometries.
MetalizationIn-house Au, Pt, Pd, Ti, W, Cu deposition for microwave antenna structures, bond pads, and integrated micro-coils.
Laser Cutting & ShapingDiamond shaping for resonator / microwave waveguide integration.
Surface FunctionalizationConsultation available on hydroxyl, carboxyl, and amine terminations analogous to Krüger’s protocol.

Engineering Support

The research described here represents a frontier where NVC physics intersects biology, requiring careful material selection to balance spin coherence, particle size, and surface chemistry. 6CCVD’s in-house PhD engineering team provides direct consultation on:

  • Selecting SCD, PCD, or BDD grades for analogous NV-based quantum sensing projects.
  • Specifying nitrogen concentration and vacancy density for target T2 performance.
  • Co-designing metalization stacks (e.g., Ti/Pt/Au) for integrated microwave delivery and fluorescence readout.
  • Wafer dicing and packaging strategies compatible with cryogenic or room-temperature ODMR rigs.

For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

Abstract The development of sensors to estimate physical properties, and their temporal and spatial variation, has been a central driving force in scientific breakthroughs. In recent years, nanosensors based on quantum measurements, such as nitrogen-vacancy centres (NVCs) in nanodiamonds, have been attracting much attention as ultrastable, sensitive, accurate and versatile physical sensors for quantitative cellular measurements. However, the nanodiamonds currently available for use as sensors have diameters of several tens of nanometres, much larger than the usual size of a protein. Therefore, their actual applications remain limited. Here we show that NVCs in an aggregation of 5-nm-sized detonation-synthesized nanodiamond treated by Krüger’s surface reduction (termed DND-OH) retains the same characteristics as observed in larger diamonds. We show that the negative charge at the NVC are stabilized, have a relatively long T2 spin relaxation time of up to 4 μs, and are applicable to thermosensing, one-degree orientation determination and nanometric super-resolution imaging. Our results clearly demonstrate the significant potential of DND-OH as a physical sensor. Thus, DND-OH will raise new possibilities for spatiotemporal monitoring of live cells and dynamic biomolecules in individual cells at single-molecule resolution.