Antireflection coating of diamond elements of power optics for CO2 lasers
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2018-11-12 |
| Journal | Quantum Electronics |
| Authors | P. A. Pivovarov, Vladimir Pavelyev, В. А. Сойфер, K. V. Cherepanov, В. И. Анисимов |
| Institutions | Image Processing Systems Institute, National Research Nuclear University MEPhI |
| Citations | 5 |
Abstract
Section titled “Abstract”A technology of deposition of a single-layer PbF2 coating, antireflecting for the CO2 laser radiation, on diamond substrates is developed. As substrates, use is made of plates of polycrystalline CVD diamond. The transmission coefficient of diamond plates with two-side coating attains 98.5 % - 99 %. The measured laser-induced damage threshold of such plates under normal environment conditions for the pulsed (τ ∼ 100 ns) and continuous-wave radiation of CO2 lasers amounts to 250 and 4 MW cm-2, respectively. These values are comparable with the thresholds of the diamond substrate damage. The increase in the damage threshold of the AR coating under continuous-wave irradiation to 5.5 MW cm-2 is found in the case of preliminary multiple irradiation of samples by weaker laser pulses. This effect can be explained by the pollutant removal from the surface of the film without its damage (laser cleaning effect).