Skip to content

Boron-doped diamond - current progress and challenges in view of electroanalytical applications

MetadataDetails
Publication Date2018-12-15
JournalAnalytical Methods
AuthorsKateryna Muzyka, Jianrui Sun, Tadesse Haile Fereja, Yixiang Lan, Wei Zhang
InstitutionsChangchun Institute of Applied Chemistry, University of Chinese Academy of Sciences
Citations230

This review examines the current status (from 2016 to December 2018) of the electroanalytical application of boron-doped diamond (BDD), in view of its advantages and challenges for electroanalytical applications.