Quantum dots formed in three-dimensional Dirac semimetal Cd$_3$As$_2$ nanowires
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2018-12-16 |
| Journal | LSU Digital Commons (Louisiana State University) |
| Authors | Minkyung Jung, Kenji Yoshida, M. B. A. Jalil, Naoto Nagaosa, Jungpil Seo |
Abstract
Section titled āAbstractāWe demonstrate quantum dot (QD) formation in three-dimensional Dirac semimetal Cd${3}$As${2}$ nanowires using two electrostatically tuned p$-$n junctions with a gate and magnetic fields. The linear conductance measured as a function of gate voltage under high magnetic fields is strongly suppressed at the Dirac point close to zero conductance, showing strong conductance oscillations. Remarkably, in this regime, the Cd${3}$As${2}$ nanowire device exhibits Coulomb diamond features, indicating that a clean single QD forms in the Dirac semimetal nanowire. Our results show that a p$-$type QD can be formed between two n$-$type leads underneath metal contacts in the nanowire by applying gate voltages under strong magnetic fields. Analysis of the quantum confinement in the gapless band structure confirms that p$-$n junctions formed between the p$-$type QD and two neighboring n$-$type leads under high magnetic fields behave as resistive tunnel barriers due to cyclotron motion, resulting in the suppression of Klein tunneling. The p$-$type QD with magnetic field-induced confinement shows a single hole filling. Our results will open up a route to quantum devices such as QDs or quantum point contacts based on Dirac and Weyl semimetals.