Weak Magnetic Field Resonance Effects in Diamond with Nitrogen-Vacancy Centers

MetadataDetails
Publication Date2018-12-01
JournalSemiconductors
AuthorsD. S. Filimonenko, V. M. YasinskiÄ­, А. П. ŠŠøŠ·Š¾Š²Ń†ŠµŠ², S. Ya. Kilin
InstitutionsNational Academy of Sciences of Belarus, B.I. Stepanov Institute of Physics
Citations6

The photoluminescence intensity of the ensemble of NV centers in diamond at weak magnetic field was studied. Two resonances were revealed in the region of weak magnetic fields: the first resonance with a width of the order of 20 G, and the second resonance with a width of the order of 180 G. The presence of these optical resonances makes it possible to propose a new concept for creating magnetic field sensors based on a diamond with an ensemble of NV centers without the use of a microwave field.