A Comparative Study of Surface Modification effects of Femtosecond and Nanosecond Laser on CVD Diamond Tools during Sharpening Processing
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Journal | Conference on Lasers and Electro-Optics |
| Authors | Xiaoxu Liu, Kohei Natsume, Satoru Maegawa, Fumihiro ITOIGAWA, Shingo Ono |
| Institutions | IMRA America (United States), Nagoya Institute of Technology |
Abstract
Section titled āAbstractāIn this study sharpening processing with femtosecond laser was innovatively performed on CVD diamond tools. Furthermore, surface modification effects of femtosecond and nanosecond laser in sharpening processing on CVD diamond were compared with Raman spectroscopy.