Luminescence landscapes of nitrogen-vacancy centers in diamond - quasi-localized vibrational resonances and selective coupling
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Journal | Journal of Materials Chemistry C |
| Authors | Zhicheng Su, Zeyang Ren, Yitian Bao, Xiangzhou Lao, Jinfeng Zhang |
| Institutions | Shenzhen University, University of Hong Kong |
| Citations | 32 |
Abstract
Section titled āAbstractā77 K micro-photoluminescence spectrum, room-temperature near-field photoluminescence image, and a local atomic arrangement of the nitrogen-vacancy (NV) center in diamond.