Photonic Integrated Circuits with Multiplexed Quantum Memories for Quantum Networks
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Authors | Matthew E. Trusheim, Michael Walsh, Eric Bersin, Noel Wan, Donggyu Kim |
| Institutions | Massachusetts Institute of Technology |
Abstract
Section titled āAbstractāAtom-like quantum emitters in diamond have emerged as leading spin-photon interfaces for quantum networks. This talk discusses the development of chip-based architectures to control large numbers of such artificial atoms for applications in quantum networks and modular quantum computing.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2019 - APS March Meeting 2019