Surface modification of polycrystalline CVD diamond films with femtosecond laser
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Journal | Conference on Lasers and Electro-Optics |
| Authors | Kohei Natsume, Xiaoxu Liu, Satoru Maegawa, Fumihiro ITOIGAWA, Shingo Ono |
| Institutions | IMRA America (United States), Nagoya Institute of Technology |
Abstract
Section titled āAbstractāThe surface modification of CVD diamond irradiated with femtosecond laser of different fluences has been studied and analyzed with Raman spectroscopy. Through comparing with DLC coating processed equally, this improved crystallinity mechanism has been discussed.