The influence of polygonal cavity on fracture behaviour of concrete
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2019-01-01 |
| Journal | Procedia Structural Integrity |
| Authors | Michal VyhlĂdal, Jan KlusĂĄk |
| Institutions | Brno University of Technology, Czech Academy of Sciences, Institute of Physics of Materials |
| Citations | 2 |
Abstract
Section titled âAbstractâIn this work, the influence of polygonal cavity on fracture behaviour of cement composite (concrete) is investigated. Specimens of the nominal dimensions 40 Ă 40 Ă 160 mm with polygonal cavity of 8 Ă 8 Ă 40 mm were provided with an initial central edge notch with a depth 12 mm, which was made by diamond blade saw. To determine the influence of polygonal cavity on fracture behaviour, fracture tests were conducted via three-point bending. The aim of this work is to analyse the behaviour of such specimen by means of finite element method (FEM) principles in Ansys, Inc. software. For this reason, a simplified 2D model was created for plane strain conditions and based on the fracture test configuration. The crack propagation assessment was based on generalized fracture mechanics approaches using a criterion of an average value of tangential stress determined in dependence on the polar angle θ. Results of numerical analysis indicates that the actual crack depth must be greater than it supposed. In other words, diamond blade saw damage the specimen more than expected.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2006 - Finite fracture mechanics: a coupled stress and energy failure criterion [Crossref]
- 1963 - On the Crack Extension in Plates Under Plane Loading and Transverse Shear [Crossref]
- 1957 - Analysis of Stresses and Strains near the End of a Crack Traversing a Plate [Crossref]
- 2007 - Crack initiation criteria for singular stress concentrations: Part I: A universal assessment of singular stress concentrations
- 2007 - Crack initiation criteria for singular stress concentrations: Part II: Stability of sharp and bi-material notches
- 2008 - A comparison of two direct methods of generalized stress intensity factor calculations of bi-material notches [Crossref]
- 2013 - The influence of discontinuity and orthotropy of fracture toughness on conditions of fracture initiation in singular stress concentrators [Crossref]