Determination of light elements C, N, O in various minerals and synthetic compounds using X-ray microanalysis
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-03-29 |
| Journal | Industrial laboratory Diagnostics of materials |
| Authors | И. М. Куликова, O. A. Nabelkin |
| Institutions | Institute of Mineralogy, Geochemistry and Crystallochemistry of Rare Elements |
| Citations | 3 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Objective: Development of an optimized methodology for X-ray spectral microanalysis (RSMA) of light elements (C, N, O) in various minerals and synthetic compounds, including ultrafine diamonds and carbon filamentous fibers.
- Core Challenge: Establishing optimal conditions for the excitation and registration of Kα-lines of light elements, which are strongly influenced by chemical bonding and matrix absorption effects.
- Instrumentation: Modernized Camebax-microbeam microanalyzer (France) with wavelength dispersion, utilizing an ODPB pseudo-crystal analyzer (2d = 99.98 Å) and an inclined spectrometer with a thin polypropylene window.
- Key Finding — Chemical Bonding Effect: The position and shape of the carbon Kα-line depend heavily on the chemical bond type—shifting to shorter wavelengths and narrowing substantially in carbonates compared to covalent diamond and graphite structures.
- Stability Innovation: Sample beam stability was enhanced by employing a raster mode (5-10 µm) and sample translation within a 100 × 100 µm² area, reducing relative standard deviation from 3.5% (point mode) to 0.83% (translated raster mode).
- Detection Limits Achieved: Carbon detection at 0.10 wt.%; oxygen detection ranging 0.39-0.90 wt.% in carbonates and 0.75 wt.% in nanodiamond colloid-grown samples.
- Validation: Successfully analyzed variscite (AlPO₄·2H₂O) and augelite (Al₂PO₄(OH)₃), achieving H₂O content of 22.32 wt.% (theoretical: 22.81 wt.%) and OH-group content of 26.91 wt.% (theoretical: 25.52 wt.%).
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Accelerating Voltage | 10 | kV | Optimal balance between surface contribution and absorption corrections |
| Beam Current | 90 - 120 | nA | Operating range for C, N, O analysis |
| C Kα Energy | 277 | eV | Analytical line for carbon |
| N Kα Energy | 392.4 | eV | Analytical line for nitrogen |
| O Kα Energy | 524.9 | eV | Analytical line for oxygen |
| Exposure Time (C) | 10 | s | Standard acquisition time |
| Exposure Time (N) | 100 | s | Extended due to high absorption in carbon matrix |
| Exposure Time (O) | 30 | s | Standard acquisition time |
| Raster Size | 5 - 10 | µm | Stability enhancement mode |
| Sample Translation Area | 100 × 100 | µm² | Maximum displacement for stability |
| Crystal Analyzer | ODPB | — | 2d = 99.98 Å |
| μ(C; O Kα) | 12,400 | cm²/g | Absorption coefficient of O by C |
| μ(C; N Kα) | 25,500 | cm²/g | Absorption coefficient of N by C |
| μ(N; O Kα) | 17,300 | cm²/g | Absorption coefficient of O by N |
| μ(Si; B Kα) | 84,000 | cm²/g | Reference for boron absorption |
| Detection Limit (C) | 0.10 | wt.% | In carbonates |
| Detection Limit (O) | 0.39 - 0.90 | wt.% | Range across rhodocrosite, kutnahorite, calcite |
| Detection Limit (O) | 0.75 | wt.% | In nanodiamond colloid samples |
| RSD (Point Mode) | 3.5 | % | Relative standard deviation |
| RSD (Raster 10×10 µm²) | 1.75 | % | Improved stability mode |
| RSD (Translated Raster 30×30 µm²) | 0.83 | % | Best stability mode |
| Peak Shift (CaCO₃ vs Diamond) | 0.17 | eV | Carbon Kα shift to shortwave region |
| Satellite Peak Position | ~14.8 | eV | Distance from main carbon maximum (longwave side) |
Key Methodologies
Section titled “Key Methodologies”- Instrument Setup: Modernized Camebax-microbeam WDS microanalyzer with ODPB pseudo-crystal (2d = 99.98 Å) and inclined spectrometer with thin polypropylene window.
- Operating Conditions Selection: Accelerating voltage set at 10 kV—sufficiently high to reduce surface defect contribution while preventing excessive absorption corrections; beam current maintained at 90-120 nA.
- Reference Standard Preparation: Ultrafine diamonds, synthetic cubic BN, and Fe₂O₃ embedded in epoxy resin pucks, coated with thin conductive carbon film to prevent charging.
- Signal Discrimination: Differential amplitude discrimination mode employed to filter higher-order reflection interference lines.
- Background Measurement Protocol: Background intensity measured adjacent to analytical lines—linear approximation for C and O regions, polynomial approximation for N region.
- Stability Enhancement Protocol:
- Raster mode (5-10 µm) for continuous analysis
- Sample translation within 100 × 100 µm² area for extended runs
- Carbon intensity measured within first 10 seconds of analysis
- Concentration Calculation: PAP program with B.L. Henke absorption coefficients; corrections via selection of absorption coefficients from comparison of K-ratios at two accelerating voltages.
- Integrated Intensity Correction: Applied ζ-correction factor (S/I ratio) to account for chemical bonding influence on spectral line shape.
- Stoichiometric Validation: Mineral formula coefficients verified against theoretical values within ±0.05 tolerance.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials
Section titled “Applicable Materials”The research methodology for characterizing light elements (C, N, O) in diamond and carbon-based materials directly aligns with several 6CCVD offerings:
- Optical Grade Single Crystal Diamond (SCD): Ideal as reference standards for X-ray microanalysis given its well-defined sp³ covalent bonding and known chemical purity. Our SCD plates (up to 125mm, thickness 0.1µm-500µm) provide the uniform crystalline structure necessary for reliable Kα-line measurements.
- Polycrystalline Diamond (PCD): Particularly relevant for this research, as the study specifically addresses analysis of ultrafine diamonds and polycrystalline aggregates. Our PCD capabilities match the micron-sized grain samples analyzed.
- Boron-Doped Diamond (BDD): For researchers extending this work to nitrogen-doped or boron-doped diamond characterization, our heavy and light boron doping options provide controlled dopant concentration for calibration standards.
Customization Potential
Section titled “Customization Potential”The paper’s use of conductive substrates (In and Be) and custom sample preparation (epoxy mounting, carbon film coating) highlights several customization opportunities:
- Custom Metallization: 6CCVD offers in-house metallization with Au, Pt, Pd, Ti, W, and Cu—critical for sample preparation in electron beam analysis. Thin-film conductive coatings (Au or Pt) can be applied to diamond substrates to enhance charge dissipation during microanalysis.
- Laser Cutting Services: Diamond samples of specific geometries can be custom-cut to fit specialized sample holders or to provide test specimens within defined µm-scale raster areas.
- Thickness Customization: For researchers requiring thin-film diamond standards, our SCD and PCD thickness range (0.1µm-500µm) accommodates varied analytical requirements—from bulk analysis to surface-layer characterization.
- Substrate Options: Diamond substrates up to 10mm thickness available for specialized sample mounting configurations.
Engineering Support
Section titled “Engineering Support”The complexity of light-element analysis in diamond matrices—particularly the absorption corrections (μ(C; O Kα) = 12,400 cm²/g) and chemical bonding effects discussed in this paper—requires careful material selection. 6CCVD’s in-house PhD team can assist with:
- Material selection guidance for diamond reference standards
- Recommendations on crystal orientation and surface preparation
- Consultation on doping levels for synthetic diamond calibration samples
- Technical support for integrating diamond materials into electron microprobe workflows
For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
The goal of the study is developing of the methodology of X-ray microanalysis of light elements C, N and O which are jointly present in various minerals and synthetic compounds, including ultrafine diamonds, carbon filamentous fibers, etc. An accelerating voltage of 10 kV high enough to reduce the contribution of the sample surface to the intensity of the lines, and at the same time prevent from the overestimation of the corrections for the line absorption was used. The beam current ranged within 90 - 120 nA. The lines of nitrogen and oxygen are particularly strongly absorbed by carbon. The background intensity is measured near the line. In the region of Kα lines of C and O, the background changes linearly, while for oxygen exhibits a large slope. The shape of continuous X-ray spectrum from the sample at 10 kV in the region of the nitrogen line can be approximated by a polynomial dependence. We used a differential mode of the amplitude discrimination of the signal. It is shown that the position and shape of the carbon line depends on the type of the chemical bond: from covalent (diamond, graphite) to a more ionic bond with oxygen (carbonates). Wide in diamond and graphite Kα lines are shifted in carbonates to the shortwave region and substantially narrowed. An additional maximum appears due to admixing of the wave functions of 2p electrons of carbon to the wave functions of 2s electrons of oxygen. The errors related to the influence of the type of chemical bond on the shape of the spectra can be avoided by the analysis of the integrated intensities. In some cases, the resistance of the samples to the impact of the electron beam is increased by the raster mode of size 5-8 micron or by moving the sample within the area ~100 x 100 pm 2 . Calculation of the concentrations was carried out in the PAP program using B. L. Henke absorption coefficients. Some errors in the correction factors for the line absorption are usually corrected by selecting the absorption coefficients. The detection limit of carbon is 0.10 % wt. and for oxygen in carbonates it ranges within 0.39 - 0.90 % wt., whereas in the samples grown from nano-diamond colloids attains 0.75 wt. %.