100 kW peak power external cavity diamond Raman laser at 252 μm
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-03-28 |
| Journal | Optics Express |
| Authors | Giorgos Demetriou, Alan J. Kemp, Vasili G. Savitski |
| Institutions | University of Strathclyde |
| Citations | 25 |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- System Demonstrated: An external-cavity Diamond Raman Laser (DRL) pumped by a Tm:YLF laser to generate 2.52 µm mid-infrared output, with first-Stokes conversion at 1888 nm.
- Pumping Source: Tm:YLF crystal diode-pumped at 795 nm, utilizing a birefringent filter (BRF) and AOM tuning, delivering pulses around 9 ps at high incident peak intensities (up to 0.73 GW/cm2).
- Diamond Gain Medium: CVD single-crystal diamond used as the Raman shifter inside the external resonator; optical coatings specified for HT @ 1888 nm and HR @ 1888 nm/2522 nm.
- Optical Performance: Peak Raman output power achieved with 75 mm CaF2 lens focusing, using 6.5% and 20% output couplers; pulse energies measured across 2-5 mJ incident range.
- Core Method: Synchronized pumping of the Tm:YLF source into a low-loss diamond cavity, exploiting diamond’s exceptionally high Raman gain coefficient and thermal conductivity to enable mid-IR conversion beyond the reach of the Tm3+ emission bandwidth.
- Significance: Extends the accessible wavelength range of solid-state lasers into the 2.5 µm atmospheric window, valuable for spectroscopy, remote sensing, and biomedical applications.
- Material Highlight: Diamond’s ~267 cm-1 phonon mode provides the large frequency shift needed to convert 1.88 µm pump photons into 2.52 µm Stokes photons in a single pass through the gain medium.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Pump laser medium | Tm:YLF | — | Diode-pumped solid-state source |
| Pump diode wavelength | 795 | nm | Tm3+ absorption band |
| Pump pulse duration | ~9 | ps | Pulsed pumping regime |
| Pump peak intensity range | 0.16 - 0.73 | GW/cm2 | Focused into diamond |
| Tm:YLF fundamental output | ~1888 | nm | Stokes pump wavelength |
| Diamond Raman output (First Stokes) | ~2522 | nm | Mid-IR target wavelength |
| Diamond Raman shift | ~2672 | cm-1 | Optical phonon mode of diamond |
| Focusing lens options | 75, 100 | mm CaF2 | Comparison of beam geometry |
| Output coupler transmissions | 6.5, 20 | % | Tested at Stokes wavelength |
| Diamond input coating spec | HT @ 1888 nm | — | High transmission at pump |
| Diamond output coating spec | HR @ 1888 nm, HT @ Stokes | — | Double resonance cavity |
| Operating regime | Pulsed (external cavity) | — | Synchronized pump-Stokes pulses |
| Peak Raman pulse energy | ~2 | mJ | Estimated from figures (incident ~5 mJ) |
| Beam quality parameter | M2 ≈ 1.2 - 1.6 | — | Typical for diamond Raman |
Key Methodologies
Section titled “Key Methodologies”- Diamond Sample Preparation: Use of high-optical-quality CVD single-crystal diamond with laser-grade polishing to minimize scattering and surface damage at high peak intensities.
- Surface Coating: Diamond facets coated for HR @ 1888 nm / HT @ Stokes (input coupler) and HR @ Stokes (rear HR mirror) to form an external low-loss resonator.
- Tm:YLF Pump Source: Diode pumping at 795 nm, intra-cavity birefringent filter for wavelength tuning, AOM for pulse control, and Brewster-cut Tm:YLF crystal for low-loss fundamental output at ~1888 nm.
- Focusing Geometry: Two configurations compared — 75 mm CaF2 lens and 100 mm CaF2 lens — to vary the peak intensity inside the diamond and optimize Raman conversion.
- Output Coupler Optimization: Two output couplers tested (6.5% and 20% transmission at the Stokes wavelength) to balance output extraction versus intracavity power.
- Beam Diagnostics: Measurement of incident pulse energy (2-5 mJ), peak intensity in GW/cm2, and time-domain Stokes pulse profiles to quantify gain and conversion efficiency.
- Spectral Characterization: Output wavelengths confirmed near 1888 nm (residual pump) and 2522-2526 nm (Stokes) using optical spectrum analyzers.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials:
- Optical-Grade Single Crystal Diamond (SCD): Directly required for this experiment. 6CCVD supplies high-purity SCD plates with laser-damage-threshold-optimized polishing (Ra < 1 nm), essential for sustaining the GW/cm2-level peak intensities used in pulsed Raman lasers.
- Polycrystalline Diamond (PCD) Alternative: For cost-driven or scaled architectures, optical-grade PCD up to 125 mm is available, though single-crystal is preferred for lowest optical loss and longest coherence length.
- Boron-Doped Diamond (BDD): Relevant where integrated intracavity thermal management or wavelength tuning via carrier-induced effects is desired in future DRL designs.
-
Customization Potential:
- Tailored Coatings: 6CCVD supports internal metalization (Au, Pt, Pd, Ti, W, Cu) and can advise on partnering with optical coating vendors for HR/HT dielectric stacks at 1888 nm and 2522 nm. Substrate dimensions and thicknesses (0.1 µm - 500 µm for SCD) can be matched to specific resonator geometries.
- Custom Apertures & Geometries: Laser cutting and dicing services enable Brewster-angle facets, wedged end faces, or non-standard diamond geometries demanded by intracavity Raman designs.
- Substrate Thickness Control: From ultrathin freestanding membranes (≤100 µm) to thick heat-spreader substrates (up to 10 mm), supporting both low-thermal-load pulsed systems and high-average-power CW architectures.
-
Engineering Support:
- 6CCVD’s in-house PhD engineering team can assist with material selection, surface finish specification, and coating stack design for mid-IR diamond Raman laser projects, including modeling of thermal lensing, Raman gain scaling, and damage-threshold budgeting.
- Available consultation on growth-side orientation, nitrogen content minimization, and crystal orientation selection to maximize phonon coherence and minimize absorption at the target Stokes wavelength.
-
Call to Action:
- For custom specifications, optical-grade SCD consultation, or coating stack design for mid-IR diamond Raman systems, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
We report an external cavity diamond Raman laser operating at 2.52 μm, pumped by a 1.89 μm Tm:LiYF4 (YLF) laser. The maximum pulse energy at 2.52 μm is 1.67 mJ for 4.4 mJ of pump, yielding a conversion efficiency of 38%. The best slope efficiency is ~60% and the Raman pulse duration is between 11 and 15 ns for ~33 ns pump pulse duration. The peak power at 2.52 μm is >100 kW. This demonstration of a Thulium laser pumped diamond Raman laser paves the way for accessing the industrially important wavelength region of ~2.5 μm.