Diamond Phononic Crystal Spin-Mechanical Resonators with Spectrally-Stable Nitrogen Vacancy Centers
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-05-05 |
| Journal | Conference on Lasers and Electro-Optics |
| Authors | Ignas Lekavicius, Thein Oo, Hailin Wang |
| Institutions | University of Oregon |
Abstract
Section titled āAbstractāWe report the design and fabrication of GHz diamond spin-mechanical resonators embedded in a two-dimensional phononic crystal lattice. Spectrally-stable nitrogen vacancy centers are observed after a soft-etching surface treatment.