Controlled Assembly of an Ultrafast Single-Photon Source

MetadataDetails
Publication Date2019-05-05
JournalConference on Lasers and Electro-Optics
AuthorsOksana Makarova, Simeon Bogdanov, Xiaohui Xu, Deesha Shah, Aleksandr S. Baburin
InstitutionsPurdue University West Lafayette, Institute of Theoretical and Applied Electrodynamics

We demonstrate a technique for highly controllable assembly of single-photon sources coupled to plasmonic nanoantennas with optimal emitter positioning on the nanoscale, resulting in fluorescence decay rates beyond 10 GHz in single nitrogen-vacancy centers. Ā© 2019 The Author(s)