Miniature Diamond-Based Fiber Optic Pressure Sensor with Dual Polymer-Ceramic Adhesives
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2019-05-13 |
| Journal | Sensors |
| Authors | Hyungdae Bae, Ayush Giri, Fikunwa O. Kolawole, Amin Azimi, Aaron D. Jackson |
| Institutions | Howard University, Joint Quantum Institute |
| Citations | 7 |
Abstract
Section titled âAbstractâDiamond is a good candidate for harsh environment sensing due to its high melting temperature, Youngâs modulus, and thermal conductivity. A sensor made of diamond will be even more promising when combined with some advantages of optical sensing (i.e., EMI inertness, high temperature operation, and miniaturization). We present a miniature diamond-based fiber optic pressure sensor fabricated using dual polymer-ceramic adhesives. The UV curable polymer and the heat-curing ceramic adhesive are employed for easy and reliable optical fiber mounting. The usage of the two different adhesives considerably improves the manufacturability and linearity of the sensor, while significantly decreasing the error from the temperature cross-sensitivity. Experimental study shows that the sensor exhibits good linearity over a pressure range of 2.0-9.5 psi with a sensitivity of 18.5 nm/psi (R2 = 0.9979). Around 275 °C of working temperature was achieved by using polymer/ceramic dual adhesives. The sensor can benefit many fronts that require miniature, low-cost, and high-accuracy sensors including biomedical and industrial applications. With an added antioxidation layer on the diamond diaphragm, the sensor can also be applied for harsh environment applications due to the high melting temperature and Youngâs modulus of the material.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 1996 - Recent progress in fibre optic low-coherence interferometry [Crossref]
- 2014 - Chronology of Fabry-Perot Interferometer Fiber-Optic Sensors and Their Applications: A Review [Crossref]
- 2002 - Novel MEMS Pressure and Temperature Sensors Fabricated on Optical Fibers [Crossref]
- 2013 - Compressible fiber optic micro-Fabry-Pérot cavity with ultra-high pressure sensitivity [Crossref]
- 2015 - Fiber-tip gas pressure sensor based on dual capillaries [Crossref]
- 2005 - Ultra-miniature fiber-optic pressure sensor using white light interferometry [Crossref]
- 2005 - Miniature all-silica fiber optic pressure and acoustic sensors [Crossref]
- 2005 - Miniature fiber-optic pressure sensor with a polymer diaphragm [Crossref]