Surface modification of polycrystalline CVD diamond films with femtosecond laser

MetadataDetails
Publication Date2019-05-05
JournalConference on Lasers and Electro-Optics
AuthorsKohei Natsume, Xiaoxu Liu, Satoru Maegawa, Fumihiro ITOIGAWA, Shingo Ono
InstitutionsIMRA America (United States), Nagoya Institute of Technology

The surface modification of CVD diamond irradiated with femtosecond laser of different fluences has been studied and analyzed with Raman spectroscopy. Through comparing with DLC coating processed equally, this improved crystallinity mechanism has been discussed. Ā© 2019 The Author(s)