Efficient Fabrication of High‐Density Ensembles of Color Centers via Ion Implantation on a Hot Diamond Substrate

MetadataDetails
Publication Date2024-07-08
JournalAdvanced Physics Research
AuthorsElena Nieto Hernández, Greta Andrini, Andreo Crnjac, Marko Brajković, Fabio Picariello
InstitutionsRudjer Boskovic Institute, Polytechnic University of Turin
Citations7

Abstract Nitrogen‐vacancy (NV) centers in diamonds are one of the most promising systems for quantum technologies, including quantum metrology and sensing. A promising strategy for the achievement of high sensitivity to external fields relies on the exploitation of large ensembles of NV centers, whose fabrication by ion implantation is upper limited by the amount of radiation damage introduced in the diamond lattice. In this work an approach is demonstrated to increase the density of NV centers upon the high‐fluence implantation of MeV N 2+ ions on a hot target substrate (>550 °C). The results show that with respect to room‐temperature implantation, the high‐temperature process increases the vacancy density threshold required for the irreversible conversion of diamond to a graphitic phase, thus enabling to achieve higher density ensembles. Furthermore, the formation efficiency of color centers is investigated on diamond substrates implanted at varying temperatures with MeV N 2+ and Mg + ions revealing that the formation efficiency of both NV centers and magnesium‐vacancy (MgV) centers increases with the implantation temperature.