Toward Novel Coherence Protection and Sensing Techniques - Closed Counter Interaction Using a Single Spin

MetadataDetails
Publication Date2019-05-05
JournalConference on Lasers and Electro-Optics
AuthorsMark Kasperczyk, Johannes Kƶlbl, Arne Barfuss, Patrick Maletinsky
InstitutionsUniversity of Basel

By studying Nitrogen Vacancy (NV) centers embedded in diamond cantilevers, we show that the coupling between the cantilever and the NV leads to novel coherent population dynamics when combined with two microwave driving fields.