Carbon-titanium based multilayer nanostructures obtained by TVA method
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-09-03 |
| Authors | V. Ciupină, C.P. Lungu, Rodica Vlădoiu, G. Prodan, Corneliu Porosniccu |
| Institutions | Ovidius University, National Institute for Laser Plasma and Radiation Physics |
| Citations | 2 |
Abstract
Section titled “Abstract”C-Ti multilayer nanostructures were deposed by Thermionic Vacuum Arc (TVA) technology. The layers consisting of about 100nm Carbon base layer and seven 40nm alternatively T i and C layers were deposed on Silicon substrates. The thickness of such a multilayer structure was up to 500nm. On the other hand, in order to obtain C-Ti multilayer structures with variable thickness and different percentages in C and T i of layers, a 20nm thick C layer was first deposed on Si substrate and then seven T i-C layers, each of these having different thickness of up to 40nm were deposed. To perform the successively layers with various thickness were changed the discharge parameters for C and T i plasma sources to obtain the desirable thickness. By changing of substrate temperature between room temperature and 300°C and on the other hand the bias voltage up to −700V , different batches of samples were obtained for this study. To characterize microstructure properties of as prepared C-Ti multilayer structures were used Electron Microscopy techniques (TEM, SEM, STEM), X-Ray Photoelectron Spectroscopy, Raman Spectroscopy and RBS techniques. The measurements reveal the content of diamond-like sp<sup>3</sup> and graphite-like sp<sup>2</sup> ; the ratio sp<sup>3</sup>/sp<sup>2</sup> increases when the bias voltage increases. Also, HRTEM and SAED patterns reveal an increase of amount and size of TiC nanocrystals with the increase of energy of Ti and C ions determined by increase of anode potential. For providing reliable quantitative information regarding the composition and the elements depth profile, RBS studies were performed using the 3MV Tandem Accelerator with specialized RBS spectrum simulation program SIRMA. Raman measurement reveal that peaks appear at around 250, 340, 420, 610, 740, 1340 and 1530−1567cm<sup>−1</sup> , suggesting mixtures of TiC, Ti<sub>3</sub>C<sub>2</sub>O<sub>2</sub> and Ti<sub>3</sub>C<sub>2</sub> and at 1340, 1560cm<sup>−1</sup> , the characteristic D an G peaks of disordered carbon. The characterstic peaks of Ti<sub>3</sub>C<sub>2</sub>O<sub>2</sub> and Ti<sub>3</sub>C<sub>2</sub> have vibrational modes at 347, 730 and 621cm<sup>−1</sup> respectively, peaks at 260 and 420cm<sup>−1</sup> correspond to TiC. The shift shown in the spectra of the samples may occurs owing to the mechanical stress. To characterize the electrical conductive properties, the electrical surface resistance versus temperature have been measured, and then the electrical conductivity. Using the Wiedeman-Frantz law was calculated the thermal conductivity, which increase with increase of the temperature, according to the decrease in the proportion of TiC phase.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2006 - Stress reduction behavior in metal-incorporated amorphous carbon films: first-principles approach